General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.02 g/cm³ Show Material materials with Densidad of 1.02 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 200 % Show Material materials with Elongación of 200 % | ISO 527-1/-2 | 50mm/min |
Elongation at yield | 23.0 °C | 32 % Show Material materials with Elongation at yield of 32 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 32 MPa Show Material materials with Límite elástico of 32 MPa | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 0.85 GPa Show Material materials with Módulo de flexión of 0.85 GPa | ISO 178 |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 45 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 45 °C | ISO 75-1/-2 | |
Temperatura de fusión | 215 °C Show Material materials with Temperatura de fusión of 215 °C | ISO 11357-1/-3 | 18°F/min | |
Inflamabilidad | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |