General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.14 g/cm³ Show Material materials with Densidad of 1.14 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.37 [-] Show Material materials with Coeficiente de Poisson of 0.37 [-] | |
Elongación | 23.0 °C | 50 % Show Material materials with Elongación of 50 % | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 84 MPa Show Material materials with Límite elástico of 84 MPa | ISO 527-1/-2 |
Módulo elástico | 23.0 °C | 3 GPa Show Material materials with Módulo elástico of 3 GPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 6 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 5 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 5 kJ/m² | ISO 180/1A |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 220 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 220 °C | ISO 75-1/-2 | |
Heat deflection temperature, 1.80 MPa | 75 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 75 °C | ISO 75-1/-2 | |
Temperatura de fusión | 263 °C Show Material materials with Temperatura de fusión of 263 °C | ISO 11357-1/-3 | 18°F/min | |
Inflamabilidad | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.05%, Melt Temperature Optimum: 290°C, Min. melt temperature: 280°C, Max. melt temperature: 300°C, Max. screw tangential speed: 0.4m/s, Mold Temperature Optimum: 70°C, Min. mold temperature: 50°C, Max. mold temperature: 90°C, Hold pressure range: 50-100MPa, Hold pressure time: 4s/mm, Ejection temperature: 190°C |