General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1 g/cm³ Show Material materials with Densidad of 1 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.45 [-] Show Material materials with Coeficiente de Poisson of 0.45 [-] | |
Elongación | 23.0 °C | 100 % Show Material materials with Elongación of 100 % | ISO 527-1/-2 | 50mm/min |
Elongation at yield | 23.0 °C | 13 % Show Material materials with Elongation at yield of 13 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 32.2 MPa Show Material materials with Límite elástico of 32.2 MPa | ISO 527-1/-2 |
Módulo elástico | 23.0 °C | 1.08 GPa Show Material materials with Módulo elástico of 1.08 GPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -6.0 °C | 15 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | ISO 179/1eA |
23.0 °C | 40 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 40 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Izod no entallado | -30.0 °C | 13 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 13 kJ/m² | ISO 180/1A |
23.0 °C | 27 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 27 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Calor específico | 23.0 °C | 2700 J/(kg·K) Show Material materials with Calor específico of 2700 J/(kg·K) | of melt | ||
Heat deflection temperature, 0.45 MPa | 85 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 85 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 46 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 46 °C | ISO 75-1/-2 | |||
Temperatura de fusión | 218 °C Show Material materials with Temperatura de fusión of 218 °C | ISO 11357-1/-3 | 18°F/min | |||
Inflamabilidad | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Technological properties