General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.07 g/cm³ Show Material materials with Densidad of 1.07 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.39 [-] Show Material materials with Coeficiente de Poisson of 0.39 [-] | |
Elongación | 23.0 °C | 500 % Show Material materials with Elongación of 500 % | min. | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 3.5 % Show Material materials with Elongation at yield of 3.5 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 58 MPa Show Material materials with Límite elástico of 58 MPa | ISO 527-1/-2 |
Módulo elástico | 23.0 °C | 2.14 GPa Show Material materials with Módulo elástico of 2.14 GPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 6 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | ISO 179/1eA |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Technological properties
Property |
---|