Zytel® PC310 NC010

Want to keep this datasheet? Save it now in your required format

Description

Zytel® PC310 NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the healthcare industry.PREMIUM CONTROL for HEALTHCARE APPLICATIONSThis product is manufactured according to Good Manufacturing Practice (GMP) principles and generally accepted in food contact applications in Europe and the USA when meeting applicable use conditions. This product is also tested against ISO 10993-5 and -11 and selected parts of USP Class VI and US FDA drug and device master files (DMF and MAF) have been established. For details, individual compliance statements are available from your DuPont representative.

Equivalent Materials

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueComment

Absorción de agua

23.0 °C

8.5 %

Show Material materials with Absorción de agua of 8.5 %

Sim. to ISO 62 | 80mil

Densidad

23.0 °C

1.14 g/cm³

Show Material materials with Densidad of 1.14 g/cm³

ISO 1183

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

23.0 °C

0.37 [-]

Show Material materials with Coeficiente de Poisson of 0.37 [-]

Dureza Rockwell M

23.0 °C

79 [-]

Show Material materials with Dureza Rockwell M of 79 [-]

ISO 2039-2

Elongación

23.0 °C

25 %

Show Material materials with Elongación of 25 %

ISO 527-1/-2

Elongation at yield

23.0 °C

4.5 %

Show Material materials with Elongation at yield of 4.5 %

ISO 527-1/-2

Hardness, Rockwell R

23.0 °C

121 [-]

Show Material materials with Hardness, Rockwell R of 121 [-]

ISO 2039-2

Límite elástico

23.0 °C

82 MPa

Show Material materials with Límite elástico of 82 MPa

ISO 527-1/-2

Módulo de flexión

23.0 °C

2.8 GPa

Show Material materials with Módulo de flexión of 2.8 GPa

ISO 178

Módulo elástico

23.0 °C

3.1 GPa

Show Material materials with Módulo elástico of 3.1 GPa

ISO 527-1/-2

Resistencia al choque, ensayo Charpy entallado

-6.0 °C

4.5 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy entallado of 4.5 kJ/m²

ISO 179/1eA

23.0 °C

5.5 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy entallado of 5.5 kJ/m²

ISO 179/1eA

Resistencia al choque, ensayo Charpy no entallado

-6.0 °C

400 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 400 kJ/m²

No Break @ 23°C, ISO 179/1eU

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

23.0 °C

2790 J/(kg·K)

Show Material materials with Calor específico of 2790 J/(kg·K)

of melt

Coeficiente de dilatación térmica

23.0 °C

1E-4 1/K

Show Material materials with Coeficiente de dilatación térmica of 1E-4 1/K

ISO 11359-1/-2

Coeficiente de dilatación térmica transversal

23.0 °C

1.1E-4 1/K

Show Material materials with Coeficiente de dilatación térmica transversal of 1.1E-4 1/K

ISO 11359-1/-2

Difusividad térmica

23.0 °C

0 mm²/s

Show Material materials with Difusividad térmica of 0 mm²/s

Heat deflection temperature, 0.45 MPa

200 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 200 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

70 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 70 °C

ISO 75-1/-2

Temperatura de fusión

262 °C

Show Material materials with Temperatura de fusión of 262 °C

ISO 11357-1/-3 | 18°F/min

Temperatura de reblandecimiento Vicat

240 °C

Show Material materials with Temperatura de reblandecimiento Vicat of 240 °C

ISO 306 | 90°F/h, 11 lbf

Temperatura de transición del vidrio

60 °C

Show Material materials with Temperatura de transición del vidrio of 60 °C

ISO 11357-1/-2 | 18°F/min

Inflamabilidad

Burning Behav. at 60mil nom. thickn.: V-2 class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: V-2 class, Thickness tested: 0.7 mm, Oxygen index: 28 %

Eléctrico

PropertyTemperatureValueComment

Constante dieléctrica, 1 MHz

23.0 °C

3.5 [-]

Show Material materials with Constante dieléctrica, 1 MHz of 3.5 [-]

IEC 62631-2-1

Constante dieléctrica, 100 Hz

23.0 °C

3.8 [-]

Show Material materials with Constante dieléctrica, 100 Hz of 3.8 [-]

IEC 62631-2-1

Dissipation factor, 100Hz

23.0 °C

8E-3 [-]

Show Material materials with Dissipation factor, 100Hz of 8E-3 [-]

IEC 62631-2-1

Dissipation factor, 1MHz

23.0 °C

0.02 [-]

Show Material materials with Dissipation factor, 1MHz of 0.02 [-]

IEC 62631-2-1

Rigidez dieléctrica

23.0 °C

32 kV/mm

Show Material materials with Rigidez dieléctrica of 32 kV/mm

IEC 60243-1

Volume resistivity

23.0 °C

1.00E+14 Ω·cm

Show Material materials with Volume resistivity of 1.00E+14 Ω·cm

IEC 62631-3-1

Índice de seguimiento comparativo

23.0 °C

600 V

Show Material materials with Índice de seguimiento comparativo of 600 V

IEC 60112

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

1.4 %

Show Material materials with Contracción of 1.4 %

ISO 294-4, 2577

Contracción transversal

23.0 °C

1.4 %

Show Material materials with Contracción transversal of 1.4 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 290°C, Min. melt temperature: 280°C, Max. melt temperature: 300°C, Max. screw tangential speed: 0.4m/s, Mold Temperature Optimum: 70°C, Min. mold temperature: 50°C, Max. mold temperature: 90°C, Hold pressure range: 50-100MPa, Hold pressure time: 4s/mm, Ejection temperature: 190°C