General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 1.1 % Show Material materials with Absorción de agua of 1.1 % | at equlibrium for 65% RH |
100.0 °C | 3 % Show Material materials with Absorción de agua of 3 % | at equlibrium for 65% RH | |
Densidad | 23.0 °C | 1.36 g/cm³ Show Material materials with Densidad of 1.36 g/cm³ | |
Densidad relativa | 23.0 °C | 1.36 [-] Show Material materials with Densidad relativa of 1.36 [-] |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 8 % Show Material materials with Elongación of 8 % |
Hardness, Rockwell R | 23.0 °C | 111 [-] Show Material materials with Hardness, Rockwell R of 111 [-] |
Módulo de flexión | 23.0 °C | 8.48 GPa Show Material materials with Módulo de flexión of 8.48 GPa |
Resistencia a la tracción | 23.0 °C | 145 MPa Show Material materials with Resistencia a la tracción of 145 MPa |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 247 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 247 kJ/m² |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor latente de fusión | 39 J/g Show Material materials with Calor latente de fusión of 39 J/g | 24% crystallinity | |
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | for -30 to 50°C |
Conductividad térmica | 23.0 °C | 0.19 W/(m·K) Show Material materials with Conductividad térmica of 0.19 W/(m·K) | |
Temperatura de flexión bajo carga | 178.85 °C Show Material materials with Temperatura de flexión bajo carga of 178.85 °C | ||
Temperatura de fusión | 187.85 °C Show Material materials with Temperatura de fusión of 187.85 °C | ||
Temperatura de transición del vidrio | 41.85 °C Show Material materials with Temperatura de transición del vidrio of 41.85 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 3.1 [-] Show Material materials with Constante dieléctrica, 1 MHz of 3.1 [-] | Dry |
Dissipation factor, 1MHz | 23.0 °C | 0.04 [-] Show Material materials with Dissipation factor, 1MHz of 0.04 [-] | Dry |
Rigidez dieléctrica | 23.0 °C | 45 kV/mm Show Material materials with Rigidez dieléctrica of 45 kV/mm |
Technological properties
Property | ||
---|---|---|
Application areas | Tubing, hoses, and pipes for automotive, trucking, industrial, and petroleum production applications. Examples are heavy truck airbrake tubing, automotive fuel lines, and submarine flexible pipes for offshore oil production. Thermoplastic powder coatings for industrial, transportation, and retail items are prepared in a Nylon 11 base. Nylon 11 is being used in a variety of food-contact applications, including sausage casing, beverage tubing, and reusable kitchen devices. | |
Fillers | 43% Glass Fiber |