General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 1.27 - 1.43 g/cm³ Show Material materials with Densidad of 1.27 - 1.43 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 59 J/m Show Material materials with Impact strength, Izod notched, ASTM of 59 J/m | ASTM D256 |
Módulo elástico | 23.0 °C | 3.19 GPa Show Material materials with Módulo elástico of 3.19 GPa | ASTM D638 |
Resistencia a la tracción | 23.0 °C | 104 MPa Show Material materials with Resistencia a la tracción of 104 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 360.85 - 366.85 °C Show Material materials with Temperatura de fusión of 360.85 - 366.85 °C | DSC |
Temperatura de transición del vidrio | 153.85 °C Show Material materials with Temperatura de transición del vidrio of 153.85 °C | DSC: 151.85°C |
Technological properties
Property |
---|