General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.43 % Show Material materials with Absorción de agua of 0.43 % | 24h |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Shore D | 23.0 °C | 89 [-] Show Material materials with Dureza Shore D of 89 [-] |
Impact strength, Izod notched, ASTM | 23.0 °C | 88 J/m Show Material materials with Impact strength, Izod notched, ASTM of 88 J/m |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 521 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 521 J/m |
Módulo de flexión | 23.0 °C | 13.97 GPa Show Material materials with Módulo de flexión of 13.97 GPa |
Resistencia a la flexión | 23.0 °C | 264 MPa Show Material materials with Resistencia a la flexión of 264 MPa |
Resistencia a la tracción | 23.0 °C | 211.7 MPa Show Material materials with Resistencia a la tracción of 211.7 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Conductividad térmica | 23.0 °C | 0.18 W/(m·K) Show Material materials with Conductividad térmica of 0.18 W/(m·K) | |
Heat deflection temperature, 1.80 MPa | 233.85 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 233.85 °C | ASTM D648 | |
Temperatura de transición del vidrio | 224.85 °C Show Material materials with Temperatura de transición del vidrio of 224.85 °C | Forced oscillation dynamic-mechanical analysis | |
Temperatura máx. de funcionamiento | 217.85 °C Show Material materials with Temperatura máx. de funcionamiento of 217.85 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Constante dieléctrica | 23.0 °C | 3.5 [-] Show Material materials with Constante dieléctrica of 3.5 [-] |
Resistividad eléctrica | 23.0 °C | 1.00E+15 Ω·m Show Material materials with Resistividad eléctrica of 1.00E+15 Ω·m |
Óptico
Property | Value |
---|---|
Índice de refracción | 1.55 [-] Show Material materials with Índice de refracción of 1.55 [-] |
Acústico
Property | Temperature | Value |
---|---|---|
Velocidad del sonido longitudinal | 23.0 °C | 2260 m/s Show Material materials with Velocidad del sonido longitudinal of 2260 m/s |
Technological properties
Property | ||
---|---|---|
Application areas | Medical and household appliances that are sterilizable by hot air and steam such as corrosion-resistant piping. Also used in electric and electronic applications such as television components. Used as membranes for reverse gas streams and gas separation. | |
Fillers | 30% Carbon Fiber |