Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 12 - 15 % Show Material materials with Elongación of 12 - 15 % |
Límite elástico | 23.0 °C | 210 - 250 MPa Show Material materials with Límite elástico of 210 - 250 MPa |
Resistencia a la tracción | 23.0 °C | 440 - 460 MPa Show Material materials with Resistencia a la tracción of 440 - 460 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | General: Gas valves and fittings, fasteners, pump trim, gears, locks, heavy-duty electrical connectors, marine hardware, transmission components, safety tools and decorative metalwork | |
Corrosion properties | A very good corrosion resistance but not as high as CZ114. | |
General machinability | Readily machinable alloy |