BS C110 / Cu-OFE Oxygen-free Copper

View suppliers (9)
Want to keep this datasheet? Save it now in your required format

Description

C110 (Cu-OFE) is the purest grade of oxygen-free copper, with a 99.99% copper content. With much tighter limits on impurities than other grades, C110 offers the highest electrical and thermal conductivity values available from a commercially available copper alloy and is not susceptible to embrittlement when hardened. Specified for electronic applications requiring freedom from harmful impurities and oxide which can impair and contaminate electronic devices, C110 also has high ductility. It shows the following features and properties:


  • Excellent electrical conductivity
  • Retention of properties at elevated temperatures
  • Outstanding thermal conductivity
  • Freedom from hydrogen embrittlement
  • Readily cold worked
  • Related Standards

    Equivalent Materials

    Los datos sobre este material han sido proporcionados por Matmatch.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    Propiedades

    Chemical properties

    PropertyValueComment

    Cobre

    99.99 %

    Show Material materials with Cobre of 99.99 %

    min.

    Technological properties

    Property
    Application areas

    General: Components for vacuum devices, switches, interrupters, deposition units, components for superconductive magnets, electron tubes including anodes, fins and collectors, glass-to-metal seals, wave guide tubes and linear accelerators

    Cold Forming

    Easily cold worked