Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 140 [-] Show Material materials with Dureza Brinell of 140 [-] |
Dureza Vickers | 23.0 °C | 140 [-] Show Material materials with Dureza Vickers of 140 [-] |
Elongación | 23.0 °C | 20 % Show Material materials with Elongación of 20 % |
Límite elástico | 23.0 °C | 400 MPa Show Material materials with Límite elástico of 400 MPa |
Resistencia a la tracción | 23.0 °C | 450 MPa Show Material materials with Resistencia a la tracción of 450 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical: Switchgear components, circuit breaker parts, rotating electrical machinery, electrical and thermal conductors;Chemical processing: Turbine generators, current-carrying arms and shafts for process plants;Other: Resistance welding, electrodes, shafts, electrode holders, seam welding wheels and flash or butt welding dies |