General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.22 g/cm³ Show Material materials with Densidad of 8.22 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 313 - 354 [-] Show Material materials with Dureza Brinell of 313 - 354 [-] |
Elongación | 23.0 °C | 12 - 17 % Show Material materials with Elongación of 12 - 17 % |
Estricción | 23.0 °C | 15 % Show Material materials with Estricción of 15 % |
Límite elástico Rp 0,2 | 23.0 °C | 827 - 1034 MPa Show Material materials with Límite elástico Rp 0,2 of 827 - 1034 MPa |
Módulo elástico | 23.0 °C | 204 GPa Show Material materials with Módulo elástico of 204 GPa |
Resistencia a la tracción | 23.0 °C | 1034 - 1276 MPa Show Material materials with Resistencia a la tracción of 1034 - 1276 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.35E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.35E-5 1/K | |
Conductividad térmica | 23.0 °C | 14.2 W/(m·K) Show Material materials with Conductividad térmica of 14.2 W/(m·K) | for 0-200°C |
Temperatura de fusión | 1260 - 1335 °C Show Material materials with Temperatura de fusión of 1260 - 1335 °C |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Material materials with Permeabilidad magnética relativa of 1 [-] |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 % Show Material materials with Aluminio of 0.5 % |
Cromo | 19 % Show Material materials with Cromo of 19 % |
Hierro | 18 - 18.5 % Show Material materials with Hierro of 18 - 18.5 % |
Molibdeno | 3 % Show Material materials with Molibdeno of 3 % |
Niobio | 5 % Show Material materials with Niobio of 5 % |
Níquel | 53 % Show Material materials with Níquel of 53 % |
Titanio | 0.9 % Show Material materials with Titanio of 0.9 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Fasteners, valves, choke stems, down-hole tooling, cryogenic storage tanks and pump bodies;Aerospace: Jet engine components, rocket motors and thrust reversers;Power generation: Nuclear reactor parts, gas turbine components, nuclear fuel element spacers, containment vessels and valves;Other: Hot extrusion tooling | |
Corrosion properties | Excellent corrosion resistance | |
Hot forming | It can be hot worked between 985-1150°C. |