Medidas
Property | Value |
---|---|
Espesor | 0.13 mm Show Material materials with Espesor of 0.13 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 150 % Show Material materials with Elongación of 150 % | ISO 527 |
Elongación transversal | 23.0 °C | 150 % Show Material materials with Elongación transversal of 150 % | ISO 527 |
Módulo elástico | 23.0 °C | 2.3 GPa Show Material materials with Módulo elástico of 2.3 GPa | ISO 527 |
Módulo elástico transversal | 23.0 °C | 2.3 GPa Show Material materials with Módulo elástico transversal of 2.3 GPa | ISO 527 |
Resistencia a la tracción | 23.0 °C | 120 MPa Show Material materials with Resistencia a la tracción of 120 MPa | ISO 527 |
Resistencia a la tracción transversal | 23.0 °C | 120 MPa Show Material materials with Resistencia a la tracción transversal of 120 MPa | ISO 527 |
Eléctrico
Technological properties
Property | ||
---|---|---|
Application areas | Electrical insulation, pressure sensitive tapes, printed circuit substrates, high temperature labels, washers in high speed motors, washers in mobile phone hinges, flexible surface heaters, aerospace insulation, pressure sensor membranes, acoustic speaker diaphragms, capacitors, composites, proven temperature resistance to use of lead free solders | |
Certifications | APTIV® film is FDA and EU approved for food contact and is RoHS and 3A Sanitary Standards compliant. | |
Other | The key features are: High heat resistance, excellent tribological properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent barrier properties, excellent acoustic properties, high purity, lightweight, recyclable, easy to process | |
Processing methods | Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. |