Medidas
Property | Value |
---|---|
Espesor | 0.1 mm Show Material materials with Espesor of 0.1 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 200 % Show Material materials with Elongación of 200 % | ISO 527 |
Elongación transversal | 23.0 °C | 200 % Show Material materials with Elongación transversal of 200 % | ISO 527 |
Módulo elástico | 23.0 °C | 1.6 GPa Show Material materials with Módulo elástico of 1.6 GPa | ISO 527 |
Módulo elástico transversal | 23.0 °C | 1.6 GPa Show Material materials with Módulo elástico transversal of 1.6 GPa | ISO 527 |
Resistencia a la tracción | 23.0 °C | 120 MPa Show Material materials with Resistencia a la tracción of 120 MPa | ISO 527 |
Resistencia a la tracción transversal | 23.0 °C | 120 MPa Show Material materials with Resistencia a la tracción transversal of 120 MPa | ISO 527 |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de transición del vidrio | 143 °C Show Material materials with Temperatura de transición del vidrio of 143 °C |
Eléctrico
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace insulation, electrical insulation, acoustic speaker diaphragms, thermoforming of thin wall parts, composites | |
Certifications | APTIV 2000 film is approved for Food Contact Use: APTIV 2000 film is compliant with the compositional requirements of FDA 21 CFR 177.2415. APTIV 2000 film is compliant with the framework regulation (EC) No. 1935/2004/EC and commission directive 2002/72/EC and the amendments up to 2005/79/EC. APTIV 2000 film is fully compliant with the 3-A Sanitary Standards. APTIV film 2000 complies with the requirements of RoHS European Directive 2002/95/EC and can be used to manufacture products compliant with the same directive. APTIV 2000 film is inherently halogen-free in accordance with IEC61249-2-21. | |
Other | The key features are: High heat resistance, excellent Flexural fatigue properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties, high purity, lightweight, recyclable, easy to process. | |
Processing methods | Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. APTIV 2000 film can easily be subjected to a range of secondary process operations, which allow designers and engineers to obtain the benefits of APTIV film properties in a variety of forms: Surface treatment, adhesion, coatings, slitting, die cutting and stamping, thermal lamination, heat welding and heat sealing, metallisation, laser marking and machining, thermoforming, printing |