General
Mecánica
Property | Value |
---|---|
Dureza Shore D | 70.0 [-] Show Material materials with Dureza Shore D of 70.0 [-] |
Elongación | 30.0 % Show Material materials with Elongación of 30.0 % |
Impact strength, Izod unnotched, ASTM | 20.0 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 20.0 J/m |
Módulo de flexión | 2.0 GPa Show Material materials with Módulo de flexión of 2.0 GPa |
Resistencia a la flexión | 65.0 MPa Show Material materials with Resistencia a la flexión of 65.0 MPa |
Resistencia a la tracción | 40 MPa Show Material materials with Resistencia a la tracción of 40 MPa |
Aplicaciones térmicas
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 8 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 8 g/10min | 160°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Straw, tube | |
Certifications | Food Contact: Halal | |
Processing methods | 1. Purge the machine using LDPE/HDPE material at original processing temperature. 2. Lower the temperature to 130 -150°C. 3. Purge the ICBP Bio Resin EVO grade at temperature of 125 - 145°C. 4. Properly adjust according to the conditions of machine and finished product. |