General
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 120.0 °C | 4 % Show Material materials with Contracción of 4 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Contracción transversal | 120.0 °C | 2 % Show Material materials with Contracción transversal of 2 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Densidad | 20.0 °C | 0.68 g/cm³ Show Material materials with Densidad of 0.68 g/cm³ | |
Densidad superficial | 20.0 °C | 2.38E-3 - 3.2E-3 g/cm² Show Material materials with Densidad superficial of 2.38E-3 - 3.2E-3 g/cm² | |
Elasticidad de la película | 20.0 °C | 31.29 - 42.02 m²/kg Show Material materials with Elasticidad de la película of 31.29 - 42.02 m²/kg |
Medidas
Property | Value |
---|---|
Espesor | 0.04 - 0.05 mm Show Material materials with Espesor of 0.04 - 0.05 mm |
Dimensions | Available thicknesses: 35, 38, 47µm. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 20.0 °C | 200 % Show Material materials with Elongación of 200 % | GOST 14236, ISO 527, ASTM D882 |
Elongación transversal | 20.0 °C | 70 % Show Material materials with Elongación transversal of 70 % | GOST 14236, ISO 527, ASTM D882 |
Resistencia a la tracción | 20.0 °C | 80 MPa Show Material materials with Resistencia a la tracción of 80 MPa | GOST 14236, ISO 527, ASTM D882 |
Resistencia a la tracción transversal | 20.0 °C | 150 MPa Show Material materials with Resistencia a la tracción transversal of 150 MPa | GOST 14236, ISO 527, ASTM D882 |
Óptico
Property | Value | Comment |
---|---|---|
Transmisión lumínica | 20 - 30 [-] Show Material materials with Transmisión lumínica of 20 - 30 [-] | GOST 15875, ISO 14782, ASTM D 1003 |
Technological properties
Property | ||
---|---|---|
Application areas | High quality solvent rotogravure and flexographic direct printing, for production of fully wrapped labels for bottles, for labeling with cold and hot melt glue. | |
Friction | Kinetic coefficient of friction µ= 0.2-0.4 (GOST 27492, ISO 8295, ASTM D 1894). | |
Other | LOBA BOPP films comprise: A modified copolymer corona treated skin layer, a white opaque oriented polypropylene tie layer, a white pearl cavitated core layer of oriented polypropylene, an oriented polypropylene tie layer, a glossy non-heat-sealable, non treated skin layer with standard coefficient of friction. | |
Processing history | Treatment level: 38 mN/m (ISO 8296, ASTM D 2578). |