General
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 120.0 °C | 4 - 5 % Show Material materials with Contracción of 4 - 5 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Contracción transversal | 120.0 °C | 2 % Show Material materials with Contracción transversal of 2 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Densidad | 20.0 °C | 0.91 g/cm³ Show Material materials with Densidad of 0.91 g/cm³ | |
Densidad superficial | 20.0 °C | 1.82E-3 - 3.64E-3 g/cm² Show Material materials with Densidad superficial of 1.82E-3 - 3.64E-3 g/cm² | |
Elasticidad de la película | 20.0 °C | 27.47 - 54.95 m²/kg Show Material materials with Elasticidad de la película of 27.47 - 54.95 m²/kg |
Medidas
Property | Value |
---|---|
Espesor | 0.02 - 0.04 mm Show Material materials with Espesor of 0.02 - 0.04 mm |
Dimensions | Available thicknesses: 20, 25, 30, 35, 40µm. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 20.0 °C | 200 - 220 % Show Material materials with Elongación of 200 - 220 % | GOST 14236, ISO 527, ASTM D882 |
Elongación transversal | 20.0 °C | 70 - 80 % Show Material materials with Elongación transversal of 70 - 80 % | GOST 14236, ISO 527, ASTM D882 |
Resistencia a la tracción | 20.0 °C | 130 - 140 MPa Show Material materials with Resistencia a la tracción of 130 - 140 MPa | GOST 14236, ISO 527, ASTM D882 |
Resistencia a la tracción transversal | 20.0 °C | 230 - 250 MPa Show Material materials with Resistencia a la tracción transversal of 230 - 250 MPa | GOST 14236, ISO 527, ASTM D882 |
Óptico
Property | Value | Comment |
---|---|---|
Turbidez | 3 - 3.2 % Show Material materials with Turbidez of 3 - 3.2 % | GOST 15875, ISO 14782, ASTM D 1003 |
Technological properties
Property | ||
---|---|---|
Application areas | High quality rotogravure and flexographic solvent based printing; production of flexible packaging, requiring no fogging during packed product storage; packing lettuce, shredded vegetables, herbs, etc.; packaging for vertical VFFS and horizontal HFFS packaging machines; application temperature with packed product + 5°C; when order please specify antifog side: IN or OUT; AF side and printable side is mentioned in each roll label. | |
Friction | Kinetic coefficient of friction µ= 0.15-0.35 (GOST 27492, ISO 8295, ASTM D 1894). | |
Other | HASL BOPP films comprise: A corona treated, heat sealable skin layer with low coefficient of friction, designed for printing, a transparent, specially designed, oriented polypropylene core layer, an antifog, corona treated, heat sealable skin layer with low coefficient of friction. | |
Processing history | Treatment level: 38 mN/m (ISO 8296, ASTM D 2578) |