General
Property | Value | Related Standards | Shape |
---|---|---|---|
Densidad | 4.45 g/cm³ Show Material materials with Densidad of 4.45 g/cm³ | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Medidas
Property | Value | Related Standards | Shape |
---|---|---|---|
Diámetro | 5 mm Show Material materials with Diámetro of 5 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube |
25.4 mm Show Material materials with Diámetro of 25.4 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet | |
125 mm Show Material materials with Diámetro of 125 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet | |
130 mm Show Material materials with Diámetro of 130 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube | |
Longitud | 1000 mm Show Material materials with Longitud of 1000 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube |
5000 mm Show Material materials with Longitud of 5000 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet |
Mecánica
Property | Value | Related Standards | Shape |
---|---|---|---|
Límite elástico | 760.0 MPa Show Material materials with Límite elástico of 760.0 MPa | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Módulo elástico | 110.0 GPa Show Material materials with Módulo elástico of 110.0 GPa | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Resistencia a la tracción | 825.0 - 860.0 MPa Show Material materials with Resistencia a la tracción of 825.0 - 860.0 MPa | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Aplicaciones térmicas
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Calor específico | 560 J/(kg·K) Show Material materials with Calor específico of 560 J/(kg·K) | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube | |
Coeficiente de dilatación térmica | 7.699999999999999e-06 - 1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 7.699999999999999e-06 - 1e-05 1/K | Typical for Titanium Alpha Beta Alloy | ||
Conductividad térmica | 6.9 W/(m·K) Show Material materials with Conductividad térmica of 6.9 W/(m·K) | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube | |
Temperatura de fusión | 1500.0 - 1750.0 °C Show Material materials with Temperatura de fusión of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 5.5 - 6.5 % Show Material materials with Aluminio of 5.5 - 6.5 % | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Carbono | 0.08 Show Material materials with Carbono of 0.08 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Hierro | 0.25 Show Material materials with Hierro of 0.25 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Oxígeno | 0.13 Show Material materials with Oxígeno of 0.13 | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |
Vanadio | 3.5 - 4.5 % Show Material materials with Vanadio of 3.5 - 4.5 % | AMS 4907, AMS 4930, AMS 6932, AMS T9046, AMS T9047 | Billet, Tube |