General
Property | Value |
---|---|
Densidad | 1.28 - 1.43 g/cm³ Show Material materials with Densidad of 1.28 - 1.43 g/cm³ |
Mecánica
Property | Value | Comment | |
---|---|---|---|
Elongación | 10.0 - 90.0 % Show Material materials with Elongación of 10.0 - 90.0 % | ||
Módulo elástico | 2.3 - 2.8 GPa Show Material materials with Módulo elástico of 2.3 - 2.8 GPa | ||
Resistencia a la tracción | 70.0 - 80.0 MPa Show Material materials with Resistencia a la tracción of 70.0 - 80.0 MPa | at 5-8% strain | |
Resistencia al choque, ensayo Charpy entallado | 60.0 - 75.0 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 60.0 - 75.0 kJ/m² | ||
Resistencia al choque, ensayo Charpy no entallado | no break |
Aplicaciones térmicas
Property | Value |
---|---|
Calor específico | 1000 J/(kg·K) Show Material materials with Calor específico of 1000 J/(kg·K) |
Coeficiente de dilatación térmica | 5.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 5.5e-05 1/K |
Conductividad térmica | 0.35 W/(m·K) Show Material materials with Conductividad térmica of 0.35 W/(m·K) |
Inflamabilidad | UL 94 V0 |
Eléctrico
Property | Value |
---|---|
Constante dieléctrica | 3.4 [-] Show Material materials with Constante dieléctrica of 3.4 [-] |
3.7 [-] Show Material materials with Constante dieléctrica of 3.7 [-] | |
Resistividad eléctrica | 10000000000000 Ω·m Show Material materials with Resistividad eléctrica of 10000000000000 Ω·m |
Óptico
Property | Value |
---|---|
Transparencia | yes |
Technological properties
Property | ||
---|---|---|
Application areas | Baby bottles, surgical instrument trays, valves, dental instruments, hot water fittings | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, blow molding, extrusion, thermoforming |