General
Property | Value |
---|---|
Densidad | 1.22 - 1.23 g/cm³ Show Material materials with Densidad of 1.22 - 1.23 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 5.0 - 6.0 % Show Material materials with Elongación of 5.0 - 6.0 % | |
Módulo elástico | 11.0 - 12.0 GPa Show Material materials with Módulo elástico of 11.0 - 12.0 GPa | |
Resistencia a la tracción | 150.0 - 160.0 MPa Show Material materials with Resistencia a la tracción of 150.0 - 160.0 MPa | at 5-6% strain |
Resistencia al choque, ensayo Charpy entallado | 15.0 - 17.0 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 15.0 - 17.0 kJ/m² | |
Resistencia al choque, ensayo Charpy no entallado | 35 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 35 kJ/m² | |
85 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 85 kJ/m² |
Aplicaciones térmicas
Property | Value |
---|---|
Calor específico | 1800 J/(kg·K) Show Material materials with Calor específico of 1800 J/(kg·K) |
Coeficiente de dilatación térmica | 2.5e-05 - 7.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.5e-05 - 7.5e-05 1/K |
Conductividad térmica | 0.43 W/(m·K) Show Material materials with Conductividad térmica of 0.43 W/(m·K) |
Temperatura de fusión | 260.0 - 262.0 °C Show Material materials with Temperatura de fusión of 260.0 - 262.0 °C |
Inflamabilidad | UL 94 HB |
Óptico
Property | Value |
---|---|
Transparencia | no |
Technological properties
Property | ||
---|---|---|
Application areas | housings, sporting goods, connectors, automotive electronics | |
Fillers | 20% Carbon Fiber | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, extrusion |