General
Property | Value |
---|---|
Densidad | 1.42 - 1.47 g/cm³ Show Material materials with Densidad of 1.42 - 1.47 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 1.5 % Show Material materials with Elongación of 1.5 % | |
Módulo elástico | 100.0 - 125.0 GPa Show Material materials with Módulo elástico of 100.0 - 125.0 GPa | |
Resistencia a la tracción | 1800.0 - 2000.0 MPa Show Material materials with Resistencia a la tracción of 1800.0 - 2000.0 MPa | at 1.5% strain |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 220 °C Show Material materials with Temperatura de fusión of 220 °C |
Óptico
Property | Value |
---|---|
Transparencia | no |
Technological properties
Property | ||
---|---|---|
Application areas | Lightweight car body, structural components, sporting goods, under hood applications, housings | |
Fillers | 60% Carbon Fiber | |
Processing methods | Thermoforming, back injection molding, insert moulding |