General
Property | Value |
---|---|
Densidad | 1.72 - 1.79 g/cm³ Show Material materials with Densidad of 1.72 - 1.79 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 2.4 % Show Material materials with Elongación of 2.4 % | |
Módulo elástico | 30.0 - 46.0 GPa Show Material materials with Módulo elástico of 30.0 - 46.0 GPa | |
Resistencia a la tracción | 730.0 - 1050.0 MPa Show Material materials with Resistencia a la tracción of 730.0 - 1050.0 MPa | at 2.4% strain |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 220 °C Show Material materials with Temperatura de fusión of 220 °C |
Óptico
Property | Value |
---|---|
Transparencia | no |
Technological properties
Property | ||
---|---|---|
Application areas | Lightweight car body, under hood applications, sporting goods, car structure | |
Fillers | 60% Glass Fiber | |
Processing methods | Thermoforming, back injection molding, insert moulding |