Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Ethylene Methyl Acrylate Copolymer (EMA)
The most thermally stable of all high-pressure PE copolymers, ethyl methyl acrylate (EMA) copolymers can be processed by extrusion coating lamination, blown/cast monolayer and coextruded films, injection molding, sheet or profile extrusion, blow molding and foam extrusion. It produces soft, elastic film (under 1.0 mil thick) with good handling characteristics and without the need for additives and increases impact strength or lowers the modulus in alloys, blends or compounds
Los datos sobre este material han sido proporcionados por M-Base.
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
PETG vs PLA
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyethylene Wax: Uses and Properties
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationGeneral
Property | Value |
---|---|
Densidad | 0.925 - 1.0 g/cm³ Show Material materials with Densidad of 0.925 - 1.0 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 500.0 - 900.0 % Show Material materials with Elongación of 500.0 - 900.0 % | |
Resistencia a la tracción | 5.0 - 15.0 MPa Show Material materials with Resistencia a la tracción of 5.0 - 15.0 MPa | at 500-900% strain |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 70.0 - 100.0 °C Show Material materials with Temperatura de fusión of 70.0 - 100.0 °C |
Óptico
Property | Value |
---|---|
Transparencia | no |
Technological properties
Property | ||
---|---|---|
Application areas | Impact modifier, upholstery films, hospital drapes | |
Processing methods | Injection molding, extrusion, coating, foaming |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.