Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Poly-M-Xylylenadipamid (PAMXD6)
It is a crystalline polyamide produced by polycondensation of MXDA with adipic acid. Different from Nylon 6 and Nylon 66, Nylon-MXD6 is an aliphatic polyamide containing an aromatic ring in its main chain. Compared with Nylon 6 and Nylon 66, Nylon-MXD6 has the following favorable characteristics:
Los datos sobre este material han sido proporcionados por M-Base.
See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
Nylon Manufacturers and Suppliers
PETG vs PLA
Polyamide Nylon: Properties, Production and Applications
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationGeneral
Property | Value |
---|---|
Densidad | 1.220 g/cm³ Show Material materials with Densidad of 1.220 g/cm³ |
Mecánica
Property | Value |
---|---|
Módulo elástico | 4.7 GPa Show Material materials with Módulo elástico of 4.7 GPa |
Aplicaciones térmicas
Property | Value |
---|---|
Coeficiente de dilatación térmica | 0.000050 1/K Show Material materials with Coeficiente de dilatación térmica of 0.000050 1/K |
Temperatura de fusión | 235.0 - 240.0 °C Show Material materials with Temperatura de fusión of 235.0 - 240.0 °C |
Óptico
Property | Value |
---|---|
Transparencia | yes |
Technological properties
Property | ||
---|---|---|
Application areas | Monofilaments, food packaging, bottles, trays, cups | |
Processing methods | Injection molding, extrusion, blow molding |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.