Poly-M-Xylylenadipamid Reinforced with 30% Glass Fibers (PAMXD6+GF30)

Nombres alternativos y comerciales
Reny®, Terez
Want to keep this datasheet? Save it now in your required format

Description

It is a reinforced Poly-M-Xylylenadipamid with 30% glass fiber. The key features are:


  • Excellent mechanical strength and elastic modulus over a wide range of temperatures
  • Lower water absorption compared to commodity polyamides showing decrease in dimensional and mechanical strength change under water absorption condition
  • High heat distortion temperature, low thermal expansion coefficient, equivalent to metal alloys
  • Excellent chemical resistance against oils and organic solvents
  • Low mold shrinkage and low warpage, suitable for precise mold articles
  • Good surface finish even in high glass fiber content
  • Los datos sobre este material han sido proporcionados por M-Base.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Propiedades

    General

    PropertyValue

    Densidad

    1.42 - 1.46 g/cm³

    Show Material materials with Densidad of 1.42 - 1.46 g/cm³

    Mecánica

    PropertyValueComment

    Elongación

    2.0 - 2.5 %

    Show Material materials with Elongación of 2.0 - 2.5 %

    Módulo elástico

    11.1 - 11.8 GPa

    Show Material materials with Módulo elástico of 11.1 - 11.8 GPa

    Resistencia a la tracción

    140.0 - 185.0 MPa

    Show Material materials with Resistencia a la tracción of 140.0 - 185.0 MPa

    at 2-2.5% strain

    Resistencia al choque, ensayo Charpy entallado

    6.0 - 7.0 kJ/m²

    Show Material materials with Resistencia al choque, ensayo Charpy entallado of 6.0 - 7.0 kJ/m²

    Resistencia al choque, ensayo Charpy no entallado

    30 kJ/m²

    Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 30 kJ/m²

    50 kJ/m²

    Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m²

    Aplicaciones térmicas

    PropertyValue

    Coeficiente de dilatación térmica

    1.5e-05 - 5e-05 1/K

    Show Material materials with Coeficiente de dilatación térmica of 1.5e-05 - 5e-05 1/K

    Temperatura de fusión

    235.0 - 240.0 °C

    Show Material materials with Temperatura de fusión of 235.0 - 240.0 °C

    Inflamabilidad

    UL 94 HB

    Eléctrico

    PropertyValue

    Constante dieléctrica

    4 [-]

    Show Material materials with Constante dieléctrica of 4 [-]

    5 [-]

    Show Material materials with Constante dieléctrica of 5 [-]

    Resistividad eléctrica

    10000000000000.0 - 20000000000000.0 Ω·m

    Show Material materials with Resistividad eléctrica of 10000000000000.0 - 20000000000000.0 Ω·m

    Óptico

    PropertyValue

    Transparencia

    no

    Technological properties

    Property
    Fillers

    30% Glass Fiber

    Processing methods

    Injection molding