General
Property | Value | Comment |
---|---|---|
Densidad | 3.51 g/cm³ Show Supplier Material materials with Densidad of 3.51 g/cm³ | |
Rango de tamaño de partículas | 1 - 22 µm Show Supplier Material materials with Rango de tamaño de partículas of 1 - 22 µm | Please refer to the technological properties section below for more detailed (narrow) particle size ranges available. |
Mecánica
Property | Value |
---|---|
Dureza (en mohs) | 10 [-] Show Supplier Material materials with Dureza (en mohs) of 10 [-] |
Aplicaciones térmicas
Property | Value |
---|---|
Coeficiente de dilatación térmica | 1.1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-06 1/K |
Conductividad térmica | 600 - 4000 W/(m·K) Show Supplier Material materials with Conductividad térmica of 600 - 4000 W/(m·K) |
Eléctrico
Property | Value |
---|---|
Banda prohibida | 6 eV Show Supplier Material materials with Banda prohibida of 6 eV |
Resistividad eléctrica | 1e+12 - 1e+19 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1e+12 - 1e+19 Ω·m |
Óptico
Property | Value |
---|---|
Índice de refracción | 2 [-] Show Supplier Material materials with Índice de refracción of 2 [-] |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbono | 99 % Show Supplier Material materials with Carbono of 99 % | min. purity |
Technological properties
Property | ||||||||||||||||||||||||||||||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Application areas | SMU SmartMicron diamond powder is ideal for lapping applications requiring a high stock removal. Typical applications include lapping of sapphire, ceramics, tungsten carbide and hard metals. | |||||||||||||||||||||||||||||||||||||||||||||||||
Color | Yellowish | |||||||||||||||||||||||||||||||||||||||||||||||||
Crystal structure | Monocrystalline | |||||||||||||||||||||||||||||||||||||||||||||||||
Gradings | Standard size range: The standard size range makes this product suitable for applications with a focus on economics. The controlled upper limit ensures a uniform, scratch-free surface quality. | |||||||||||||||||||||||||||||||||||||||||||||||||
Morphology | Structured particle surface: The micro-structured, rough particle surface maximizes the material removal rate due to the numerous contact points provided between diamond particles and the work piece. | |||||||||||||||||||||||||||||||||||||||||||||||||
Particle size range table |
| |||||||||||||||||||||||||||||||||||||||||||||||||
Synthesis | Modified synthetic diamond |