General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Densidad of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Estricción | 20.0 °C | 53 % Show Material materials with Estricción of 53 % | |
540.0 °C | 44 % Show Material materials with Estricción of 44 % | ||
650.0 °C | 97 % Show Material materials with Estricción of 97 % | ||
Límite elástico | 20.0 °C | 690 MPa Show Material materials with Límite elástico of 690 MPa | |
540.0 °C | 220 MPa Show Material materials with Límite elástico of 220 MPa | ||
650.0 °C | 110 MPa Show Material materials with Límite elástico of 110 MPa | ||
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Martensitic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Martensitic Stainless Steel |
Resistencia a la tracción | 20.0 °C | 920 MPa Show Material materials with Resistencia a la tracción of 920 MPa | |
540.0 °C | 270 MPa Show Material materials with Resistencia a la tracción of 270 MPa | ||
650.0 °C | 130 MPa Show Material materials with Resistencia a la tracción of 130 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Conductividad térmica | 23.0 °C | 14 - 31 W/(m·K) Show Material materials with Conductividad térmica of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Temperatura de fusión | 1370 - 1530 °C Show Material materials with Temperatura de fusión of 1370 - 1530 °C | Typical for Martensitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.35 - 0.45 % Show Material materials with Carbono of 0.35 - 0.45 % |
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % |
Cromo | 1.85 - 2.5 % Show Material materials with Cromo of 1.85 - 2.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 91.85 - 94 % Show Material materials with Hierro of 91.85 - 94 % |
Manganeso | 0.2 - 0.4 % Show Material materials with Manganeso of 0.2 - 0.4 % |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % |
Níquel | 0.25 % Show Material materials with Níquel of 0.25 % |
Silicona | 3.6 - 4.2 % Show Material materials with Silicona of 3.6 - 4.2 % |