Acero bajo en carbono
JIS G3128 Grade E460E normalized, controlled rolledMalleable Cast Iron
SAE J158 Grade M4504 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5003 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5503 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M7002 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M8501 Liquid quenched and TemperedAcero inoxidable austenítico
SAE J775 Grade EV-16 For Mechanical Tests: ST+PAcero inoxidable martensítico
SAE J775 Grade NV-8Acero inoxidable austenítico
SAE J775 Grade EV-3Acero inoxidable austenítico
SAE J775 Grade EV-7Nickel Chromium Alloy
SAE HEV-8Acero para herramientas y maquinaria
JIS G4404 Grade SKD12Suministrada por:
2 proveedores de Matmatch
Acero para herramientas y maquinaria
JIS G4404 Grade SKD61Suministrada por:
3 proveedores de Matmatch
Nickel Chromium Molybdenum Steel
JIS G4103 Grade SNCM815Acero
SAE J775 Grade HNV-7Nickel Chromium Molybdenum Steel
JIS G4103 Grade SNCM625Nickel Chromium Molybdenum Steel
JIS G4103 Grade SNCM630Nickel Chromium Alloy
SAE HEV-2Nickel Chromium Alloy
SAE HEV-6