Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 12CrMo9-10 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoV9-10 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10216-2 Grade 12CrMo9-10 quenched and tempered (+QT)Acero
ASTM A387 Grade 22 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A542 Type A Class 2 Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A542 Type D Class 1 Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A542 Type A Class 1 Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A542 Type B Class 1 Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Acero
ASTM A387 Grade 22 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Unclassified Stainless Steel
ASTM A543 Class 1 Type B Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Unclassified Stainless Steel
ASTM A543 Class 1 Type C Quenched and TemperedSuministrada por:
1 proveedor Matmatch