General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Elongación | 17.3 % Show Material materials with Elongación of 17.3 % | Predicted Value, A200 | ||||
18.4 % Show Material materials with Elongación of 18.4 % | Predicted Value, A80 | |||||
20.3 % Show Material materials with Elongación of 20.3 % | Predicted Value, A80 Transverse | |||||
21.1 % Show Material materials with Elongación of 21.1 % | Predicted Value, A5 | |||||
21.4 % Show Material materials with Elongación of 21.4 % | Predicted Value, Transverse | |||||
22.5 % Show Material materials with Elongación of 22.5 % | Predicted Value, A50 | |||||
20 °C | 22 % Show Material materials with Elongación of 22 % | thermomechanically rolled | EN 10028-5 | Flat | ||
Estricción | 40.3 % Show Material materials with Estricción of 40.3 % | Predicted Value | ||||
44.3 % Show Material materials with Estricción of 44.3 % | Predicted Value, Transverse | |||||
Límite elástico | 254.6 MPa Show Material materials with Límite elástico of 254.6 MPa | Predicted Value, RP1 | ||||
318.5 MPa Show Material materials with Límite elástico of 318.5 MPa | Predicted Value, RP1 Transverse | |||||
357.1 MPa Show Material materials with Límite elástico of 357.1 MPa | Predicted Value, RP02 | |||||
393.4 MPa Show Material materials with Límite elástico of 393.4 MPa | Predicted Value, Transverse | |||||
453.7 MPa Show Material materials with Límite elástico of 453.7 MPa | Predicted Value, RP02 Transverse | |||||
468.2 MPa Show Material materials with Límite elástico of 468.2 MPa | Predicted Value, RP05 | |||||
494.9 MPa Show Material materials with Límite elástico of 494.9 MPa | Predicted Value, RP002 | |||||
20 °C | 345 MPa Show Material materials with Límite elástico of 345 MPa | thermomechanically rolled | EN 10028-5 | Flat | ||
20 °C | 355 MPa Show Material materials with Límite elástico of 355 MPa | thermomechanically rolled | EN 10028-5 | Flat | ||
Módulo de cizallamiento | 79.6 GPa Show Material materials with Módulo de cizallamiento of 79.6 GPa | Predicted Value | ||||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20 °C | 450 - 610 MPa Show Material materials with Resistencia a la tracción of 450 - 610 MPa | thermomechanically rolled | EN 10028-5 | Flat | |
Resistencia al cizallamiento | 558.8 MPa Show Material materials with Resistencia al cizallamiento of 558.8 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 455 J/(kg·K) Show Material materials with Calor específico of 455 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.74 1/K Show Material materials with Coeficiente de dilatación térmica of 11.74 1/K | Predicted Value |
Conductividad térmica | 38.03 W/(m·K) Show Material materials with Conductividad térmica of 38.03 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % | thermomechanically rolled | EN 10028-5 | Flat |
Azufre | 0.008 % Show Material materials with Azufre of 0.008 % | thermomechanically rolled | EN 10028-5 | Flat |
0.015 % Show Material materials with Azufre of 0.015 % | thermomechanically rolled | EN 10028-5 | Flat | |
Carbono | 0.14 % Show Material materials with Carbono of 0.14 % | thermomechanically rolled | EN 10028-5 | Flat |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % | thermomechanically rolled | EN 10028-5 | Flat |
Manganeso | 1.6 % Show Material materials with Manganeso of 1.6 % | thermomechanically rolled | EN 10028-5 | Flat |
Molibdeno | 0.2 % Show Material materials with Molibdeno of 0.2 % | thermomechanically rolled | EN 10028-5 | Flat |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % | thermomechanically rolled | EN 10028-5 | Flat |
Nitrógeno | 0.015 % Show Material materials with Nitrógeno of 0.015 % | thermomechanically rolled | EN 10028-5 | Flat |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % | thermomechanically rolled | EN 10028-5 | Flat |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | thermomechanically rolled | EN 10028-5 | Flat |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % | thermomechanically rolled | EN 10028-5 | Flat |
Vanadio | 0.1 % Show Material materials with Vanadio of 0.1 % | thermomechanically rolled | EN 10028-5 | Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |