General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Steel |
Módulo de cizallamiento | 20.0 °C | 81 GPa Show Material materials with Módulo de cizallamiento of 81 GPa | |
Módulo elástico | 20.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa | |
200.0 °C | 188 GPa Show Material materials with Módulo elástico of 188 GPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 1/K | |
Conductividad térmica | 20.0 °C | 42 W/(m·K) Show Material materials with Conductividad térmica of 42 W/(m·K) | |
100.0 °C | 39.8 W/(m·K) Show Material materials with Conductividad térmica of 39.8 W/(m·K) | ||
200.0 °C | 37.7 W/(m·K) Show Material materials with Conductividad térmica of 37.7 W/(m·K) | ||
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Steel |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.6E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.6E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Boro | 8E-4 - 5E-3 % Show Material materials with Boro of 8E-4 - 5E-3 % |
Carbono | 0.14 - 0.19 % Show Material materials with Carbono of 0.14 - 0.19 % |
Cobre | 0.4 % Show Material materials with Cobre of 0.4 % |
Cromo | 0.8 - 1.1 % Show Material materials with Cromo of 0.8 - 1.1 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1 - 1.3 % Show Material materials with Manganeso of 1 - 1.3 % |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % |