General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.2 g/cm³ Show Material materials with Densidad of 8.2 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | -269.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] |
-195.0 °C | 0.31 [-] Show Material materials with Coeficiente de Poisson of 0.31 [-] | |
27.0 °C | 0.31 [-] Show Material materials with Coeficiente de Poisson of 0.31 [-] | |
Dureza Brinell | 20.0 °C | 331 [-] Show Material materials with Dureza Brinell of 331 [-] |
Dureza Vickers | 20.0 °C | 350 [-] Show Material materials with Dureza Vickers of 350 [-] |
Elongación | 20.0 °C | 8 - 11 % Show Material materials with Elongación of 8 - 11 % |
Elongación A50 transversal | 20.0 °C | 12 % Show Material materials with Elongación A50 transversal of 12 % |
Elongación transversal | 20.0 °C | 5 % Show Material materials with Elongación transversal of 5 % |
Estricción | 20.0 °C | 15 - 20 % Show Material materials with Estricción of 15 - 20 % |
Límite elástico Rp 0,2 | 20.0 °C | 1040 - 1440 MPa Show Material materials with Límite elástico Rp 0,2 of 1040 - 1440 MPa |
200.0 °C | 1040 MPa Show Material materials with Límite elástico Rp 0,2 of 1040 MPa | |
300.0 °C | 1020 MPa Show Material materials with Límite elástico Rp 0,2 of 1020 MPa | |
400.0 °C | 1000 MPa Show Material materials with Límite elástico Rp 0,2 of 1000 MPa | |
500.0 °C | 950 - 980 MPa Show Material materials with Límite elástico Rp 0,2 of 950 - 980 MPa | |
600.0 °C | 950 MPa Show Material materials with Límite elástico Rp 0,2 of 950 MPa | |
700.0 °C | 870 MPa Show Material materials with Límite elástico Rp 0,2 of 870 MPa | |
800.0 °C | 640 MPa Show Material materials with Límite elástico Rp 0,2 of 640 MPa | |
Límite elástico transversal Rp 0,2 | 20.0 °C | 1040 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 1040 MPa |
Módulo elástico | -269.0 °C | 210.9 GPa Show Material materials with Módulo elástico of 210.9 GPa |
-195.0 °C | 212.3 GPa Show Material materials with Módulo elástico of 212.3 GPa | |
20.0 °C | 199 GPa Show Material materials with Módulo elástico of 199 GPa | |
27.0 °C | 204.1 GPa Show Material materials with Módulo elástico of 204.1 GPa | |
100.0 °C | 195 GPa Show Material materials with Módulo elástico of 195 GPa | |
200.0 °C | 190 GPa Show Material materials with Módulo elástico of 190 GPa | |
300.0 °C | 185 GPa Show Material materials with Módulo elástico of 185 GPa | |
400.0 °C | 179 GPa Show Material materials with Módulo elástico of 179 GPa | |
500.0 °C | 174 GPa Show Material materials with Módulo elástico of 174 GPa | |
600.0 °C | 167 GPa Show Material materials with Módulo elástico of 167 GPa | |
700.0 °C | 163 GPa Show Material materials with Módulo elástico of 163 GPa | |
800.0 °C | 149 GPa Show Material materials with Módulo elástico of 149 GPa | |
900.0 °C | 134 GPa Show Material materials with Módulo elástico of 134 GPa | |
Reducción de área, transversal | 20.0 °C | 8 % Show Material materials with Reducción de área, transversal of 8 % |
Resistencia a la tracción | 20.0 °C | 1270 - 1750 MPa Show Material materials with Resistencia a la tracción of 1270 - 1750 MPa |
Resistencia a la tracción transversal | 20.0 °C | 1240 MPa Show Material materials with Resistencia a la tracción transversal of 1240 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) | |
100.0 °C | 450 J/(kg·K) Show Material materials with Calor específico of 450 J/(kg·K) | ||
200.0 °C | 470 J/(kg·K) Show Material materials with Calor específico of 470 J/(kg·K) | ||
300.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | ||
400.0 °C | 520 J/(kg·K) Show Material materials with Calor específico of 520 J/(kg·K) | ||
500.0 °C | 530 J/(kg·K) Show Material materials with Calor específico of 530 J/(kg·K) | ||
600.0 °C | 560 J/(kg·K) Show Material materials with Calor específico of 560 J/(kg·K) | ||
700.0 °C | 630 J/(kg·K) Show Material materials with Calor específico of 630 J/(kg·K) | ||
800.0 °C | 640 J/(kg·K) Show Material materials with Calor específico of 640 J/(kg·K) | ||
900.0 °C | 650 J/(kg·K) Show Material materials with Calor específico of 650 J/(kg·K) | ||
Coeficiente de dilatación térmica | 100.0 °C | 1.28E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.28E-5 1/K | |
200.0 °C | 1.34E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.34E-5 1/K | ||
300.0 °C | 1.38E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.38E-5 1/K | ||
400.0 °C | 1.41E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.41E-5 1/K | ||
500.0 °C | 1.43E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.43E-5 1/K | ||
600.0 °C | 1.47E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.47E-5 1/K | ||
700.0 °C | 1.56E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.56E-5 1/K | ||
800.0 °C | 1.64E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.64E-5 1/K | ||
900.0 °C | 1.72E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.72E-5 1/K | ||
Conductividad térmica | 20.0 °C | 13 W/(m·K) Show Material materials with Conductividad térmica of 13 W/(m·K) | |
100.0 °C | 13 W/(m·K) Show Material materials with Conductividad térmica of 13 W/(m·K) | ||
200.0 °C | 14 W/(m·K) Show Material materials with Conductividad térmica of 14 W/(m·K) | ||
300.0 °C | 15 W/(m·K) Show Material materials with Conductividad térmica of 15 W/(m·K) | ||
400.0 °C | 17 W/(m·K) Show Material materials with Conductividad térmica of 17 W/(m·K) | ||
500.0 °C | 19 W/(m·K) Show Material materials with Conductividad térmica of 19 W/(m·K) | ||
600.0 °C | 21 W/(m·K) Show Material materials with Conductividad térmica of 21 W/(m·K) | ||
700.0 °C | 23 W/(m·K) Show Material materials with Conductividad térmica of 23 W/(m·K) | ||
800.0 °C | 25 W/(m·K) Show Material materials with Conductividad térmica of 25 W/(m·K) | ||
900.0 °C | 27 W/(m·K) Show Material materials with Conductividad térmica of 27 W/(m·K) | ||
Temperatura de fusión | 1200 - 1480 °C Show Material materials with Temperatura de fusión of 1200 - 1480 °C | Typical for Nickel Chromium Iron Alloy | |
Temperatura máx. de funcionamiento, largo | -250 - 700 °C Show Material materials with Temperatura máx. de funcionamiento, largo of -250 - 700 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 800000 S/m Show Material materials with Conductividad eléctrica of 800000 S/m |
Resistividad eléctrica | 20.0 °C | 1.25E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.25E-6 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.3 - 0.7 % Show Material materials with Aluminio of 0.3 - 0.7 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Boro | 2E-3 - 6E-3 % Show Material materials with Boro of 2E-3 - 6E-3 % |
Carbono | 0.02 - 0.7 % Show Material materials with Carbono of 0.02 - 0.7 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 17 - 21 % Show Material materials with Cromo of 17 - 21 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 11.33 - 24.3 % Show Material materials with Hierro of 11.33 - 24.3 % |
Manganeso | 0.35 % Show Material materials with Manganeso of 0.35 % |
Molibdeno | 2.8 - 3.3 % Show Material materials with Molibdeno of 2.8 - 3.3 % |
Niobio | 4.8 - 5.5 % Show Material materials with Niobio of 4.8 - 5.5 % |
Níquel | 50 - 55 % Show Material materials with Níquel of 50 - 55 % |
Silicona | 0.35 % Show Material materials with Silicona of 0.35 % |
Titanio | 0.7 - 1.15 % Show Material materials with Titanio of 0.7 - 1.15 % |