General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.73 g/cm³ Show Material materials with Densidad of 7.73 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] |
100.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | |
200.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | |
300.0 °C | 0.31 [-] Show Material materials with Coeficiente de Poisson of 0.31 [-] | |
400.0 °C | 0.31 [-] Show Material materials with Coeficiente de Poisson of 0.31 [-] | |
Estricción | 20.0 °C | 60 % Show Material materials with Estricción of 60 % |
Módulo de cizallamiento | 20.0 °C | 84.82 GPa Show Material materials with Módulo de cizallamiento of 84.82 GPa |
100.0 °C | 82.5 GPa Show Material materials with Módulo de cizallamiento of 82.5 GPa | |
200.0 °C | 79.57 GPa Show Material materials with Módulo de cizallamiento of 79.57 GPa | |
300.0 °C | 75.86 GPa Show Material materials with Módulo de cizallamiento of 75.86 GPa | |
400.0 °C | 72 GPa Show Material materials with Módulo de cizallamiento of 72 GPa | |
Módulo elástico | 20.0 °C | 217 - 217.99 GPa Show Material materials with Módulo elástico of 217 - 217.99 GPa |
100.0 °C | 213.2 - 215 GPa Show Material materials with Módulo elástico of 213.2 - 215 GPa | |
200.0 °C | 188 - 205.94 GPa Show Material materials with Módulo elástico of 188 - 205.94 GPa | |
300.0 °C | 164 - 198.53 GPa Show Material materials with Módulo elástico of 164 - 198.53 GPa | |
400.0 °C | 188.79 GPa Show Material materials with Módulo elástico of 188.79 GPa | |
Resistencia a la tracción | 20.0 °C | 600 MPa Show Material materials with Resistencia a la tracción of 600 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 439 J/(kg·K) Show Material materials with Calor específico of 439 J/(kg·K) | |
100.0 °C | 474 J/(kg·K) Show Material materials with Calor específico of 474 J/(kg·K) | ||
200.0 °C | 498 J/(kg·K) Show Material materials with Calor específico of 498 J/(kg·K) | ||
300.0 °C | 517 J/(kg·K) Show Material materials with Calor específico of 517 J/(kg·K) | ||
400.0 °C | 538 J/(kg·K) Show Material materials with Calor específico of 538 J/(kg·K) | ||
500.0 °C | 564 J/(kg·K) Show Material materials with Calor específico of 564 J/(kg·K) | ||
600.0 °C | 598 J/(kg·K) Show Material materials with Calor específico of 598 J/(kg·K) | ||
Coeficiente de dilatación térmica | 20.0 °C | 1.02E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.02E-5 1/K | |
100.0 °C | 1.05E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.05E-5 1/K | ||
200.0 °C | 1.09E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.09E-5 1/K | ||
300.0 °C | 1.13E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.13E-5 1/K | ||
400.0 °C | 1.16E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.16E-5 1/K | ||
500.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K | ||
600.0 °C | 1.22E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.22E-5 1/K | ||
Conductividad térmica | 20.0 °C | 25.9 W/(m·K) Show Material materials with Conductividad térmica of 25.9 W/(m·K) | |
100.0 °C | 25.3 W/(m·K) Show Material materials with Conductividad térmica of 25.3 W/(m·K) | ||
200.0 °C | 25.2 W/(m·K) Show Material materials with Conductividad térmica of 25.2 W/(m·K) | ||
300.0 °C | 25.2 W/(m·K) Show Material materials with Conductividad térmica of 25.2 W/(m·K) | ||
400.0 °C | 25.4 W/(m·K) Show Material materials with Conductividad térmica of 25.4 W/(m·K) | ||
500.0 °C | 25.7 W/(m·K) Show Material materials with Conductividad térmica of 25.7 W/(m·K) | ||
600.0 °C | 25.9 W/(m·K) Show Material materials with Conductividad térmica of 25.9 W/(m·K) | ||
Difusividad térmica | 20.0 °C | 7.6 mm²/s Show Material materials with Difusividad térmica of 7.6 mm²/s | |
100.0 °C | 6.6 mm²/s Show Material materials with Difusividad térmica of 6.6 mm²/s | ||
200.0 °C | 6.1 mm²/s Show Material materials with Difusividad térmica of 6.1 mm²/s | ||
300.0 °C | 5.8 mm²/s Show Material materials with Difusividad térmica of 5.8 mm²/s | ||
400.0 °C | 5.3 mm²/s Show Material materials with Difusividad térmica of 5.3 mm²/s | ||
500.0 °C | 4.8 mm²/s Show Material materials with Difusividad térmica of 4.8 mm²/s | ||
600.0 °C | 4.1 mm²/s Show Material materials with Difusividad térmica of 4.1 mm²/s | ||
Temperatura de fusión | 1375 - 1450 °C Show Material materials with Temperatura de fusión of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Temperatura máx. de funcionamiento, largo | 0 - 550 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 550 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 5.59E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.59E-7 Ω·m |
100.0 °C | 6.4E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.4E-7 Ω·m | |
200.0 °C | 7.32E-7 Ω·m Show Material materials with Resistividad eléctrica of 7.32E-7 Ω·m | |
300.0 °C | 8.17E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.17E-7 Ω·m | |
400.0 °C | 8.97E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.97E-7 Ω·m | |
500.0 °C | 9.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 9.74E-7 Ω·m | |
600.0 °C | 1.05E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.05E-6 Ω·m | |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.08 - 0.12 % Show Material materials with Carbono of 0.08 - 0.12 % |
Cromo | 12 - 14 % Show Material materials with Cromo of 12 - 14 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |