General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 5 % Show Material materials with Elongación of 5 % | |
Estricción | 20.0 °C | 30 % Show Material materials with Estricción of 30 % | |
Límite elástico Rp 0,2 | 20.0 °C | 1650 MPa Show Material materials with Límite elástico Rp 0,2 of 1650 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 1700 - 2000 MPa Show Material materials with Resistencia a la tracción of 1700 - 2000 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.56 - 0.64 % Show Material materials with Carbono of 0.56 - 0.64 % |
Cromo | 0.2 - 0.4 % Show Material materials with Cromo of 0.2 - 0.4 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.7 - 1 % Show Material materials with Manganeso of 0.7 - 1 % |
Silicona | 1.5 - 2 % Show Material materials with Silicona of 1.5 - 2 % |
Vanadio | 0.1 - 0.2 % Show Material materials with Vanadio of 0.1 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Features | Spring |