General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Elongación | 14.1 % Show Material materials with Elongación of 14.1 % | Predicted Value, A200 | ||||
15.2 % Show Material materials with Elongación of 15.2 % | Predicted Value, A80 | |||||
18.1 % Show Material materials with Elongación of 18.1 % | Predicted Value, Transverse | |||||
18.4 % Show Material materials with Elongación of 18.4 % | Predicted Value, A80 Transverse | |||||
20.3 % Show Material materials with Elongación of 20.3 % | Predicted Value, A5 | |||||
23.2 % Show Material materials with Elongación of 23.2 % | Predicted Value, A50 | |||||
20 °C | 17 % Show Material materials with Elongación of 17 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat | ||
Estricción | 40 % Show Material materials with Estricción of 40 % | Predicted Value | ||||
44.5 % Show Material materials with Estricción of 44.5 % | Predicted Value, Transverse | |||||
Límite elástico | 263.7 MPa Show Material materials with Límite elástico of 263.7 MPa | Predicted Value, RP1 | ||||
319.2 MPa Show Material materials with Límite elástico of 319.2 MPa | Predicted Value, RP1 Transverse | |||||
427.8 MPa Show Material materials with Límite elástico of 427.8 MPa | Predicted Value, RP02 | |||||
441.9 MPa Show Material materials with Límite elástico of 441.9 MPa | Predicted Value, Transverse | |||||
491.6 MPa Show Material materials with Límite elástico of 491.6 MPa | Predicted Value, RP02 Transverse | |||||
541.7 MPa Show Material materials with Límite elástico of 541.7 MPa | Predicted Value, RP05 | |||||
544.3 MPa Show Material materials with Límite elástico of 544.3 MPa | Predicted Value, RP002 | |||||
20 °C | 400 MPa Show Material materials with Límite elástico of 400 MPa | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat | ||
20 °C | 440 MPa Show Material materials with Límite elástico of 440 MPa | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat | ||
20 °C | 460 MPa Show Material materials with Límite elástico of 460 MPa | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat | ||
Módulo de cizallamiento | 79.8 GPa Show Material materials with Módulo de cizallamiento of 79.8 GPa | Predicted Value | ||||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20 °C | 500 - 720 MPa Show Material materials with Resistencia a la tracción of 500 - 720 MPa | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat | |
20 °C | 500 - 670 MPa Show Material materials with Resistencia a la tracción of 500 - 670 MPa | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat | ||
20 °C | 550 - 720 MPa Show Material materials with Resistencia a la tracción of 550 - 720 MPa | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat | ||
20 °C | 550 - 670 MPa Show Material materials with Resistencia a la tracción of 550 - 670 MPa | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat | ||
Resistencia al cizallamiento | 559 MPa Show Material materials with Resistencia al cizallamiento of 559 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 442.2 J/(kg·K) Show Material materials with Calor específico of 442.2 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.87 1/K Show Material materials with Coeficiente de dilatación térmica of 11.87 1/K | Predicted Value |
Conductividad térmica | 35.67 W/(m·K) Show Material materials with Conductividad térmica of 35.67 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Boro | 0.005 % Show Material materials with Boro of 0.005 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Circonio | 0.15 % Show Material materials with Circonio of 0.15 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Cromo | 1.5 % Show Material materials with Cromo of 1.5 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Manganeso | 1.7 % Show Material materials with Manganeso of 1.7 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Molibdeno | 0.7 % Show Material materials with Molibdeno of 0.7 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Niobio | 0.06 % Show Material materials with Niobio of 0.06 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Nitrógeno | 0.015 % Show Material materials with Nitrógeno of 0.015 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Níquel | 2 % Show Material materials with Níquel of 2 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Vanadio | 0.12 % Show Material materials with Vanadio of 0.12 % | quenched and tempered (+QT) | EN 10137-2, EN 10025-6 | Sheet, Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |