General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Steel |
Dureza Brinell | 20.0 °C | 140 - 240 [-] Show Material materials with Dureza Brinell of 140 - 240 [-] | |
Módulo elástico | 200.0 °C | 188 GPa Show Material materials with Módulo elástico of 188 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 - 494 J/(kg·K) Show Material materials with Calor específico of 440 - 494 J/(kg·K) | Typical for Chromium Steel |
Coeficiente de dilatación térmica | 100.0 °C | 1.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 1/K | |
Conductividad térmica | 100.0 °C | 39.8 W/(m·K) Show Material materials with Conductividad térmica of 39.8 W/(m·K) | |
200.0 °C | 37.7 W/(m·K) Show Material materials with Conductividad térmica of 37.7 W/(m·K) | ||
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Boro | 8E-4 - 5E-3 % Show Material materials with Boro of 8E-4 - 5E-3 % |
Carbono | 0.14 - 0.19 % Show Material materials with Carbono of 0.14 - 0.19 % |
Cromo | 0.8 - 1.1 % Show Material materials with Cromo of 0.8 - 1.1 % |
Fósforo | 0.03 - 0.04 % Show Material materials with Fósforo of 0.03 - 0.04 % |
Manganeso | 1 - 1.3 % Show Material materials with Manganeso of 1 - 1.3 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |