EN 10250-4 Grade X2CrNiN23-4 solution annealed (+AT)

View suppliers (10)
Want to keep this datasheet? Save it now in your required format

Description

Make X2CrNiN23-4 is comparable to X 2 CrNiN 23 4 acc. to SEW 400 :1991-02. The material is a stainless Duplex-steel of high strength and hardness and favorable resistance to general corrosion, pitting corrosion and especially to stress corrosion. Furthermore it shows resistance to intercrystalline corrosion also insensitized condition. Application for leight weight constructions of longer durability and higher reliability, for heat-exchanger and pipelines in chloride-containing media, hydraulic tubes, feeder water preheater, agitator shafts, steam heating systems.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

7.8 g/cm³

Show Material materials with Densidad of 7.8 g/cm³

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

23.0 °C

0.3 [-]

Show Material materials with Coeficiente de Poisson of 0.3 [-]

Typical for Duplex Stainless Steel

Elongación

20.0 °C

25 %

Show Material materials with Elongación of 25 %

Elongación transversal

20.0 °C

20 %

Show Material materials with Elongación transversal of 20 %

Límite elástico Rp 0,2

20.0 °C

400 MPa

Show Material materials with Límite elástico Rp 0,2 of 400 MPa

100.0 °C

330 MPa

Show Material materials with Límite elástico Rp 0,2 of 330 MPa

150.0 °C

300 MPa

Show Material materials with Límite elástico Rp 0,2 of 300 MPa

200.0 °C

280 MPa

Show Material materials with Límite elástico Rp 0,2 of 280 MPa

250.0 °C

265 MPa

Show Material materials with Límite elástico Rp 0,2 of 265 MPa

Módulo de cizallamiento

23.0 °C

77 GPa

Show Material materials with Módulo de cizallamiento of 77 GPa

Typical for Duplex Stainless Steel

Módulo elástico

20.0 °C

200 - 212 GPa

Show Material materials with Módulo elástico of 200 - 212 GPa

100.0 °C

194 - 206 GPa

Show Material materials with Módulo elástico of 194 - 206 GPa

200.0 °C

186 GPa

Show Material materials with Módulo elástico of 186 GPa

300.0 °C

180 GPa

Show Material materials with Módulo elástico of 180 GPa

Unlock all property charts

Resistencia a la tracción

20.0 °C

600 - 830 MPa

Show Material materials with Resistencia a la tracción of 600 - 830 MPa

Resistencia a la tracción transversal

20.0 °C

600 - 830 MPa

Show Material materials with Resistencia a la tracción transversal of 600 - 830 MPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

20.0 °C

500 J/(kg·K)

Show Material materials with Calor específico of 500 J/(kg·K)

Coeficiente de dilatación térmica

100.0 °C

1.3E-5 - 1.33E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 - 1.33E-5 1/K

200.0 °C

1.35E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.35E-5 1/K

300.0 °C

1.4E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K

Unlock all property charts

Conductividad térmica

20.0 °C

13.4 - 15 W/(m·K)

Show Material materials with Conductividad térmica of 13.4 - 15 W/(m·K)

100.0 °C

14.9 W/(m·K)

Show Material materials with Conductividad térmica of 14.9 W/(m·K)

Unlock all property charts

Temperatura de fusión

1375 - 1450 °C

Show Material materials with Temperatura de fusión of 1375 - 1450 °C

Typical for Duplex Stainless Steel

Temperatura máx. de funcionamiento

300 °C

Show Material materials with Temperatura máx. de funcionamiento of 300 °C

Typical for Duplex Stainless Steel

Eléctrico

PropertyTemperatureValue

Resistividad eléctrica

20.0 °C

7.85E-7 Ω·m

Show Material materials with Resistividad eléctrica of 7.85E-7 Ω·m

100.0 °C

8.44E-7 Ω·m

Show Material materials with Resistividad eléctrica of 8.44E-7 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Azufre

0.015 %

Show Material materials with Azufre of 0.015 %

Carbono

0.03 %

Show Material materials with Carbono of 0.03 %

Cobre

0.1 - 0.6 %

Show Material materials with Cobre of 0.1 - 0.6 %

Cromo

22 - 24 %

Show Material materials with Cromo of 22 - 24 %

Fósforo

0.04 %

Show Material materials with Fósforo of 0.04 %

Manganeso

2 %

Show Material materials with Manganeso of 2 %

Molibdeno

0.1 - 0.6 %

Show Material materials with Molibdeno of 0.1 - 0.6 %

Nitrógeno

0.05 - 0.2 %

Show Material materials with Nitrógeno of 0.05 - 0.2 %

Níquel

3.5 - 5.5 %

Show Material materials with Níquel of 3.5 - 5.5 %

Silicona

1 %

Show Material materials with Silicona of 1 %