General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Elongación | 17.0 % Show Material materials with Elongación of 17.0 % | Predicted Value, A80 | ||||
17.4 % Show Material materials with Elongación of 17.4 % | Predicted Value, A200 | |||||
20.7 % Show Material materials with Elongación of 20.7 % | Predicted Value, A80 Transverse | |||||
20.8 % Show Material materials with Elongación of 20.8 % | Predicted Value, Transverse | |||||
21.0 % Show Material materials with Elongación of 21.0 % | Predicted Value, A5 | |||||
24.2 % Show Material materials with Elongación of 24.2 % | Predicted Value, A50 | |||||
20 °C | 19 % Show Material materials with Elongación of 19 % | thermomechanically rolled | EN 10225 | Sheet | ||
Estricción | 39.8 % Show Material materials with Estricción of 39.8 % | Predicted Value | ||||
44.4 % Show Material materials with Estricción of 44.4 % | Predicted Value, Transverse | |||||
Límite elástico | 260 MPa Show Material materials with Límite elástico of 260 MPa | Predicted Value, RP1 | ||||
317.7 MPa Show Material materials with Límite elástico of 317.7 MPa | Predicted Value, RP1 Transverse | |||||
412.9 MPa Show Material materials with Límite elástico of 412.9 MPa | Predicted Value, RP02 | |||||
415.8 MPa Show Material materials with Límite elástico of 415.8 MPa | Predicted Value, Transverse | |||||
488 MPa Show Material materials with Límite elástico of 488 MPa | Predicted Value, RP02 Transverse | |||||
488.9 MPa Show Material materials with Límite elástico of 488.9 MPa | Predicted Value, RP05 | |||||
496.7 MPa Show Material materials with Límite elástico of 496.7 MPa | Predicted Value, RP002 | |||||
20 °C | 380 MPa Show Material materials with Límite elástico of 380 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 390 MPa Show Material materials with Límite elástico of 390 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 400 MPa Show Material materials with Límite elástico of 400 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 420 MPa Show Material materials with Límite elástico of 420 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
Módulo de cizallamiento | 79.9 GPa Show Material materials with Módulo de cizallamiento of 79.9 GPa | Predicted Value | ||||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20 °C | 480 - 660 MPa Show Material materials with Resistencia a la tracción of 480 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | |
20 °C | 480 - 640 MPa Show Material materials with Resistencia a la tracción of 480 - 640 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 500 - 660 MPa Show Material materials with Resistencia a la tracción of 500 - 660 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
20 °C | 500 - 640 MPa Show Material materials with Resistencia a la tracción of 500 - 640 MPa | thermomechanically rolled | EN 10225 | Sheet | ||
Resistencia al cizallamiento | 544.4 MPa Show Material materials with Resistencia al cizallamiento of 544.4 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 453.1 J/(kg·K) Show Material materials with Calor específico of 453.1 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.89 1/K Show Material materials with Coeficiente de dilatación térmica of 11.89 1/K | Predicted Value |
Conductividad térmica | 36.99 W/(m·K) Show Material materials with Conductividad térmica of 36.99 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.015 - 0.055 % Show Material materials with Aluminio of 0.015 - 0.055 % | thermomechanically rolled | EN 10225 | Sheet |
Antimonio | 0.01 % Show Material materials with Antimonio of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Arsénico | 0.03 % Show Material materials with Arsénico of 0.03 % | thermomechanically rolled | EN 10225 | Sheet |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Bismuto | 0.01 % Show Material materials with Bismuto of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Boro | 0.001 % Show Material materials with Boro of 0.001 % | thermomechanically rolled | EN 10225 | Sheet |
Calcio | 0.005 % Show Material materials with Calcio of 0.005 % | thermomechanically rolled | EN 10225 | Sheet |
Carbono | 0.14 % Show Material materials with Carbono of 0.14 % | thermomechanically rolled | EN 10225 | Sheet |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % | thermomechanically rolled | EN 10225 | Sheet |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % | thermomechanically rolled | EN 10225 | Sheet |
Estaño | 0.02 % Show Material materials with Estaño of 0.02 % | thermomechanically rolled | EN 10225 | Sheet |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % | thermomechanically rolled | EN 10225 | Sheet |
Manganeso | 1.65 % Show Material materials with Manganeso of 1.65 % | thermomechanically rolled | EN 10225 | Sheet |
Molibdeno | 0.25 % Show Material materials with Molibdeno of 0.25 % | thermomechanically rolled | EN 10225 | Sheet |
Niobio | 0.04 % Show Material materials with Niobio of 0.04 % | thermomechanically rolled | EN 10225 | Sheet |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Níquel | 0.7 % Show Material materials with Níquel of 0.7 % | thermomechanically rolled | EN 10225 | Sheet |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % | thermomechanically rolled | EN 10225 | Sheet |
Silicona | 0.15 - 0.55 % Show Material materials with Silicona of 0.15 - 0.55 % | thermomechanically rolled | EN 10225 | Sheet |
Titanio | 0.025 % Show Material materials with Titanio of 0.025 % | thermomechanically rolled | EN 10225 | Sheet |
Vanadio | 0.08 % Show Material materials with Vanadio of 0.08 % | thermomechanically rolled | EN 10225 | Sheet |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |