General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 - 8.94 g/cm³ Show Material materials with Densidad of 8.9 - 8.94 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | |
Dureza Vickers | 20.0 °C | 55 [-] Show Material materials with Dureza Vickers of 55 [-] | |
Elongación | 20.0 °C | 30 - 42 % Show Material materials with Elongación of 30 - 42 % | |
Elongación transversal | 20.0 °C | 33 % Show Material materials with Elongación transversal of 33 % | |
Límite elástico Rp 0,2 | 20.0 °C | 40 - 100 MPa Show Material materials with Límite elástico Rp 0,2 of 40 - 100 MPa | |
Límite elástico Rp 1,0 | 20.0 °C | 60 MPa Show Material materials with Límite elástico Rp 1,0 of 60 MPa | |
50.0 °C | 55 - 60 MPa Show Material materials with Límite elástico Rp 1,0 of 55 - 60 MPa | ||
100.0 °C | 55 MPa Show Material materials with Límite elástico Rp 1,0 of 55 MPa | ||
150.0 °C | 55 MPa Show Material materials with Límite elástico Rp 1,0 of 55 MPa | ||
Límite elástico transversal Rp 0,2 | 20.0 °C | 40 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 40 MPa | |
Límite elástico transversal Rp 1,0 | 20.0 °C | 60 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 60 MPa | |
50.0 °C | 60 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 60 MPa | ||
100.0 °C | 55 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 55 MPa | ||
150.0 °C | 55 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 55 MPa | ||
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | -253.0 °C | 138 GPa Show Material materials with Módulo elástico of 138 GPa | |
-195.0 °C | 136 GPa Show Material materials with Módulo elástico of 136 GPa | ||
-100.0 °C | 133 GPa Show Material materials with Módulo elástico of 133 GPa | ||
20.0 °C | 128 - 132 GPa Show Material materials with Módulo elástico of 128 - 132 GPa | ||
50.0 °C | 127 GPa Show Material materials with Módulo elástico of 127 GPa | ||
100.0 °C | 125 GPa Show Material materials with Módulo elástico of 125 GPa | ||
150.0 °C | 122 GPa Show Material materials with Módulo elástico of 122 GPa | ||
200.0 °C | 120 GPa Show Material materials with Módulo elástico of 120 GPa | ||
250.0 °C | 118 GPa Show Material materials with Módulo elástico of 118 GPa | ||
Resistencia a la tracción | 20.0 °C | 200 - 250 MPa Show Material materials with Resistencia a la tracción of 200 - 250 MPa | |
50.0 °C | 125 - 200 MPa Show Material materials with Resistencia a la tracción of 125 - 200 MPa | ||
100.0 °C | 200 MPa Show Material materials with Resistencia a la tracción of 200 MPa | ||
150.0 °C | 175 MPa Show Material materials with Resistencia a la tracción of 175 MPa | ||
200.0 °C | 150 MPa Show Material materials with Resistencia a la tracción of 150 MPa | ||
250.0 °C | 125 MPa Show Material materials with Resistencia a la tracción of 125 MPa | ||
Resistencia a la tracción transversal | 20.0 °C | 200 MPa Show Material materials with Resistencia a la tracción transversal of 200 MPa | |
50.0 °C | 200 MPa Show Material materials with Resistencia a la tracción transversal of 200 MPa | ||
100.0 °C | 200 MPa Show Material materials with Resistencia a la tracción transversal of 200 MPa | ||
150.0 °C | 175 MPa Show Material materials with Resistencia a la tracción transversal of 175 MPa | ||
200.0 °C | 150 MPa Show Material materials with Resistencia a la tracción transversal of 150 MPa | ||
250.0 °C | 125 MPa Show Material materials with Resistencia a la tracción transversal of 125 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | -150.0 °C | 282 J/(kg·K) Show Material materials with Calor específico of 282 J/(kg·K) | |
-50.0 °C | 361 J/(kg·K) Show Material materials with Calor específico of 361 J/(kg·K) | ||
20.0 °C | 386 J/(kg·K) Show Material materials with Calor específico of 386 J/(kg·K) | ||
100.0 °C | 393 J/(kg·K) Show Material materials with Calor específico of 393 J/(kg·K) | ||
200.0 °C | 403 J/(kg·K) Show Material materials with Calor específico of 403 J/(kg·K) | ||
300.0 °C | 415 J/(kg·K) Show Material materials with Calor específico of 415 J/(kg·K) | ||
Coeficiente de dilatación térmica | 100.0 °C | 1.68E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.68E-5 1/K | |
200.0 °C | 1.73E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.73E-5 1/K | ||
300.0 °C | 1.77E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.77E-5 1/K | ||
Conductividad térmica | 20.0 °C | 305 - 340 W/(m·K) Show Material materials with Conductividad térmica of 305 - 340 W/(m·K) | |
50.0 °C | 310 W/(m·K) Show Material materials with Conductividad térmica of 310 W/(m·K) | ||
100.0 °C | 318 W/(m·K) Show Material materials with Conductividad térmica of 318 W/(m·K) | ||
200.0 °C | 326 W/(m·K) Show Material materials with Conductividad térmica of 326 W/(m·K) | ||
300.0 °C | 334 W/(m·K) Show Material materials with Conductividad térmica of 334 W/(m·K) | ||
Temperatura de fusión | 965 - 1100 °C Show Material materials with Temperatura de fusión of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 4.30E+7 S/m Show Material materials with Conductividad eléctrica of 4.30E+7 S/m |
50.0 °C | 4.10E+7 S/m Show Material materials with Conductividad eléctrica of 4.10E+7 S/m | |
100.0 °C | 3.70E+7 S/m Show Material materials with Conductividad eléctrica of 3.70E+7 S/m | |
200.0 °C | 3.40E+7 S/m Show Material materials with Conductividad eléctrica of 3.40E+7 S/m | |
300.0 °C | 3.00E+7 S/m Show Material materials with Conductividad eléctrica of 3.00E+7 S/m | |
Resistividad eléctrica | 20.0 °C | 2.2E-8 Ω·m Show Material materials with Resistividad eléctrica of 2.2E-8 Ω·m |
50.0 °C | 2.4E-8 Ω·m Show Material materials with Resistividad eléctrica of 2.4E-8 Ω·m | |
100.0 °C | 2.7E-8 Ω·m Show Material materials with Resistividad eléctrica of 2.7E-8 Ω·m | |
200.0 °C | 2.9E-8 Ω·m Show Material materials with Resistividad eléctrica of 2.9E-8 Ω·m | |
300.0 °C | 3.3E-8 Ω·m Show Material materials with Resistividad eléctrica of 3.3E-8 Ω·m | |
Chemical properties
Property | Value |
---|---|
Cobre | 99.9 % Show Material materials with Cobre of 99.9 % |
Fósforo | 0.02 - 0.04 % Show Material materials with Fósforo of 0.02 - 0.04 % |
Plata | 0.02 % Show Material materials with Plata of 0.02 % |