General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 90 [-] Show Material materials with Dureza Vickers of 90 [-] |
Elongación | 20.0 °C | 30 - 43 % Show Material materials with Elongación of 30 - 43 % |
Elongación A50 | 20.0 °C | 33 % Show Material materials with Elongación A50 of 33 % |
Elongación transversal | 20.0 °C | 30 - 43 % Show Material materials with Elongación transversal of 30 - 43 % |
Límite elástico Rp 0,2 | 20.0 °C | 120 - 240 MPa Show Material materials with Límite elástico Rp 0,2 of 120 - 240 MPa |
Límite elástico Rp 1,0 | 50.0 °C | 140 MPa Show Material materials with Límite elástico Rp 1,0 of 140 MPa |
100.0 °C | 137 MPa Show Material materials with Límite elástico Rp 1,0 of 137 MPa | |
150.0 °C | 137 MPa Show Material materials with Límite elástico Rp 1,0 of 137 MPa | |
200.0 °C | 132 MPa Show Material materials with Límite elástico Rp 1,0 of 132 MPa | |
Límite elástico transversal Rp 0,2 | 20.0 °C | 120 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 120 MPa |
Límite elástico transversal Rp 1,0 | 20.0 °C | 140 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 140 MPa |
50.0 °C | 140 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 140 MPa | |
100.0 °C | 137 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 137 MPa | |
150.0 °C | 137 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 137 MPa | |
200.0 °C | 132 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 132 MPa | |
Módulo de cizallamiento | 20.0 °C | 37 GPa Show Material materials with Módulo de cizallamiento of 37 GPa |
Módulo elástico | -195.0 °C | 108 GPa Show Material materials with Módulo elástico of 108 GPa |
-100.0 °C | 106 GPa Show Material materials with Módulo elástico of 106 GPa | |
20.0 °C | 102 - 105 GPa Show Material materials with Módulo elástico of 102 - 105 GPa | |
50.0 °C | 100 GPa Show Material materials with Módulo elástico of 100 GPa | |
100.0 °C | 93 GPa Show Material materials with Módulo elástico of 93 GPa | |
150.0 °C | 91 GPa Show Material materials with Módulo elástico of 91 GPa | |
200.0 °C | 89 GPa Show Material materials with Módulo elástico of 89 GPa | |
250.0 °C | 83 GPa Show Material materials with Módulo elástico of 83 GPa | |
Resistencia a la tracción | 20.0 °C | 340 - 420 MPa Show Material materials with Resistencia a la tracción of 340 - 420 MPa |
Resistencia a la tracción transversal | 20.0 °C | 340 MPa Show Material materials with Resistencia a la tracción transversal of 340 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Calor específico of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Coeficiente de dilatación térmica | 200.0 °C | 2.04E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.04E-5 1/K | |
Conductividad térmica | 20.0 °C | 109 W/(m·K) Show Material materials with Conductividad térmica of 109 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.39E+7 S/m Show Material materials with Conductividad eléctrica of 1.39E+7 S/m |
Resistividad eléctrica | 20.0 °C | 7.2E-8 Ω·m Show Material materials with Resistividad eléctrica of 7.2E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 59 - 60.5 % Show Material materials with Cobre of 59 - 60.5 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.2 - 0.8 % Show Material materials with Plomo of 0.2 - 0.8 % |