EN 12163 Grade Cu-DHP H100

View suppliers (23)
Want to keep this datasheet? Save it now in your required format

Description

Cu-DHP, mat. No CW024A, is a phosphoric pure copper grade. To the comparable DIN-mark SF-Cu, mat. No 2.0090 acc. to DIN 1787 applies: The material is a deoxidized copper with Cu >= 99,9% and a high residual copper-content. Tensile strength and Brinell hardness are increasable by cold forming. SF-Cu (Cu-DHP) is hydrogen resistant and shows the lowest thermal and electrical conductivity of the pure copper materials. Processing properties: hot forming: very good cold forming: very good machinability: unfavorable hard soldering: very good soft soldering: very good gas-shielded welding: very good burnishing: very good Application: SF-Cu is the most important copper-grade for pipes due to its very good soldering and welding properties. Further application in apparatus engineering and construction trade. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.9 - 8.94 g/cm³

Show Material materials with Densidad of 8.9 - 8.94 g/cm³

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

20.0 °C

0.34 [-]

Show Material materials with Coeficiente de Poisson of 0.34 [-]

Dureza Brinell

20.0 °C

100 [-]

Show Material materials with Dureza Brinell of 100 [-]

Dureza Vickers

20.0 °C

100 - 110 [-]

Show Material materials with Dureza Vickers of 100 - 110 [-]

Módulo de cizallamiento

23.0 °C

48 GPa

Show Material materials with Módulo de cizallamiento of 48 GPa

Typical for Wrought Copper Pure / Low Alloyed Copper

Módulo elástico

-253.0 °C

138 GPa

Show Material materials with Módulo elástico of 138 GPa

-195.0 °C

136 GPa

Show Material materials with Módulo elástico of 136 GPa

-100.0 °C

133 GPa

Show Material materials with Módulo elástico of 133 GPa

20.0 °C

128 - 132 GPa

Show Material materials with Módulo elástico of 128 - 132 GPa

50.0 °C

127 GPa

Show Material materials with Módulo elástico of 127 GPa

100.0 °C

125 GPa

Show Material materials with Módulo elástico of 125 GPa

150.0 °C

122 GPa

Show Material materials with Módulo elástico of 122 GPa

200.0 °C

120 GPa

Show Material materials with Módulo elástico of 120 GPa

250.0 °C

118 GPa

Show Material materials with Módulo elástico of 118 GPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

-150.0 °C

282 J/(kg·K)

Show Material materials with Calor específico of 282 J/(kg·K)

-50.0 °C

361 J/(kg·K)

Show Material materials with Calor específico of 361 J/(kg·K)

20.0 °C

386 J/(kg·K)

Show Material materials with Calor específico of 386 J/(kg·K)

100.0 °C

393 J/(kg·K)

Show Material materials with Calor específico of 393 J/(kg·K)

200.0 °C

403 J/(kg·K)

Show Material materials with Calor específico of 403 J/(kg·K)

300.0 °C

415 J/(kg·K)

Show Material materials with Calor específico of 415 J/(kg·K)

Unlock all property charts

Coeficiente de dilatación térmica

100.0 °C

1.68E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.68E-5 1/K

200.0 °C

1.73E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.73E-5 1/K

300.0 °C

1.77E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.77E-5 1/K

Unlock all property charts

Conductividad térmica

20.0 °C

305 - 340 W/(m·K)

Show Material materials with Conductividad térmica of 305 - 340 W/(m·K)

50.0 °C

310 W/(m·K)

Show Material materials with Conductividad térmica of 310 W/(m·K)

100.0 °C

318 W/(m·K)

Show Material materials with Conductividad térmica of 318 W/(m·K)

200.0 °C

326 W/(m·K)

Show Material materials with Conductividad térmica of 326 W/(m·K)

300.0 °C

334 W/(m·K)

Show Material materials with Conductividad térmica of 334 W/(m·K)

Unlock all property charts

Temperatura de fusión

965 - 1100 °C

Show Material materials with Temperatura de fusión of 965 - 1100 °C

Typical for Wrought Copper Pure / Low Alloyed Copper

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

4.30E+7 S/m

Show Material materials with Conductividad eléctrica of 4.30E+7 S/m

50.0 °C

4.10E+7 S/m

Show Material materials with Conductividad eléctrica of 4.10E+7 S/m

100.0 °C

3.70E+7 S/m

Show Material materials with Conductividad eléctrica of 3.70E+7 S/m

200.0 °C

3.40E+7 S/m

Show Material materials with Conductividad eléctrica of 3.40E+7 S/m

300.0 °C

3.00E+7 S/m

Show Material materials with Conductividad eléctrica of 3.00E+7 S/m

Unlock all property charts

Resistividad eléctrica

20.0 °C

2.2E-8 Ω·m

Show Material materials with Resistividad eléctrica of 2.2E-8 Ω·m

50.0 °C

2.4E-8 Ω·m

Show Material materials with Resistividad eléctrica of 2.4E-8 Ω·m

100.0 °C

2.7E-8 Ω·m

Show Material materials with Resistividad eléctrica of 2.7E-8 Ω·m

200.0 °C

2.9E-8 Ω·m

Show Material materials with Resistividad eléctrica of 2.9E-8 Ω·m

300.0 °C

3.3E-8 Ω·m

Show Material materials with Resistividad eléctrica of 3.3E-8 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Cobre

99.9 %

Show Material materials with Cobre of 99.9 %

Fósforo

0.02 - 0.04 %

Show Material materials with Fósforo of 0.02 - 0.04 %

Plata

0.02 %

Show Material materials with Plata of 0.02 %