General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 14 % Show Material materials with Elongación of 14 % |
Elongation A10 | 20.0 °C | 12 % Show Material materials with Elongation A10 of 12 % |
Elongation A100 | 20.0 °C | 10 % Show Material materials with Elongation A100 of 10 % |
Elongation A11.3 | 20.0 °C | 12 % Show Material materials with Elongation A11.3 of 12 % |
Límite elástico Rp 0,2 | 20.0 °C | 180 MPa Show Material materials with Límite elástico Rp 0,2 of 180 MPa |
Módulo elástico | 20.0 °C | 150 GPa Show Material materials with Módulo elástico of 150 GPa |
Resistencia a la tracción | 20.0 °C | 420 MPa Show Material materials with Resistencia a la tracción of 420 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Calor específico of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Coeficiente de dilatación térmica | 300.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | |
Conductividad térmica | 20.0 °C | 29 W/(m·K) Show Material materials with Conductividad térmica of 29 W/(m·K) | |
Temperatura de fusión | 915 - 1240 °C Show Material materials with Temperatura de fusión of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobalto | 0.1 % Show Material materials with Cobalto of 0.1 % |
Estaño | 0.05 % Show Material materials with Estaño of 0.05 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 0.4 - 1 % Show Material materials with Hierro of 0.4 - 1 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Níquel | 30 - 32 % Show Material materials with Níquel of 30 - 32 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |