General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.25 - 8.3 g/cm³ Show Material materials with Densidad of 8.25 - 8.3 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Dureza Brinell | 20.0 °C | 130 - 220 [-] Show Material materials with Dureza Brinell of 130 - 220 [-] | |
Dureza Vickers | 20.0 °C | 130 - 200 [-] Show Material materials with Dureza Vickers of 130 - 200 [-] | |
Módulo elástico | 20.0 °C | 85 - 100 GPa Show Material materials with Módulo elástico of 85 - 100 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Conductividad térmica | 20.0 °C | 33 - 35 W/(m·K) Show Material materials with Conductividad térmica of 33 - 35 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 4.50E+6 S/m Show Material materials with Conductividad eléctrica of 4.50E+6 S/m |
Specific Electrical conductivity | 7.8 % IACS Show Material materials with Specific Electrical conductivity of 7.8 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 75 - 77 % Show Material materials with Cobre of 75 - 77 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Fósforo | 0.02 - 0.1 % Show Material materials with Fósforo of 0.02 - 0.1 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 0.05 % Show Material materials with Manganeso of 0.05 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % |
Silicona | 2.7 - 3.5 % Show Material materials with Silicona of 2.7 - 3.5 % |