EN 12166 Grade CuNi12Zn24 H200

View suppliers (9)
Want to keep this datasheet? Save it now in your required format

Description

Material CuNi12Zn24, mat. No. CW403J is an alloy of high strength and hardness. To the comparabel DIN-mark CuNi12Zn24, mat. No. 2.0730, acc. to DIN 17663 : 1983-12 applies: Strength is further increasable due to the high strain hardening capability. The material does not embrittle at low temperatures. Low electrical and thermal conductivity. The alloy is non-magnetic, corrosion resistance is better than for pure copper. Processing properties: warm forming: moderately cold forming: very good machinability: moderately hard and soft soldering: very good TIG-welding: very good burnishing: very good Application: In electrical engineering and electronics for springs, contacts, membranes as well as in precision engineering and in equipment manufacturing. In food industry, for musical instruments, glasses frames, safety keys as well as in construction trade for paneling, show-cases and stairrails.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.67 - 8.7 g/cm³

Show Material materials with Densidad of 8.67 - 8.7 g/cm³

Mecánica

PropertyTemperatureValue

Coeficiente de Poisson

20.0 °C

0.34 [-]

Show Material materials with Coeficiente de Poisson of 0.34 [-]

Dureza Vickers

20.0 °C

200 [-]

Show Material materials with Dureza Vickers of 200 [-]

Módulo elástico

20.0 °C

125 GPa

Show Material materials with Módulo elástico of 125 GPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

20.0 °C

380 J/(kg·K)

Show Material materials with Calor específico of 380 J/(kg·K)

Coeficiente de dilatación térmica

300.0 °C

1.65E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.65E-5 1/K

Conductividad térmica

20.0 °C

42 W/(m·K)

Show Material materials with Conductividad térmica of 42 W/(m·K)

Temperatura de fusión

875 - 1135 °C

Show Material materials with Temperatura de fusión of 875 - 1135 °C

Typical for Wrought Copper Nickel Silver Grade

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

4.40E+6 S/m

Show Material materials with Conductividad eléctrica of 4.40E+6 S/m

Specific Electrical conductivity

8 % IACS

Show Material materials with Specific Electrical conductivity of 8 % IACS

Chemical properties

PropertyValue

Cobre

63 - 66 %

Show Material materials with Cobre of 63 - 66 %

Estaño

0.03 %

Show Material materials with Estaño of 0.03 %

Hierro

0.3 %

Show Material materials with Hierro of 0.3 %

Manganeso

0.5 %

Show Material materials with Manganeso of 0.5 %

Níquel

11 - 13 %

Show Material materials with Níquel of 11 - 13 %

Plomo

0.03 %