General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.85 g/cm³ Show Material materials with Densidad of 8.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Dureza Vickers | 20.0 °C | 125 - 160 [-] Show Material materials with Dureza Vickers of 125 - 160 [-] | |
Elongación | 20.0 °C | 25 % Show Material materials with Elongación of 25 % | |
Elongation A10 | 20.0 °C | 20 % Show Material materials with Elongation A10 of 20 % | |
Elongation A100 | 20.0 °C | 7 - 15 % Show Material materials with Elongation A100 of 7 - 15 % | |
Límite elástico Rp 0,2 | 20.0 °C | 270 - 300 MPa Show Material materials with Límite elástico Rp 0,2 of 270 - 300 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Resistencia a la tracción | 20.0 °C | 400 - 550 MPa Show Material materials with Resistencia a la tracción of 400 - 550 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) |
Coeficiente de dilatación térmica | 100.0 °C | 1.78E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.78E-5 1/K |
200.0 °C | 1.82E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.82E-5 1/K | |
300.0 °C | 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K | |
650.0 °C | 2.06E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.06E-5 1/K | |
800.0 °C | 2.05E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.05E-5 1/K | |
Conductividad térmica | 20.0 °C | 90 W/(m·K) Show Material materials with Conductividad térmica of 90 W/(m·K) |
200.0 °C | 120 W/(m·K) Show Material materials with Conductividad térmica of 120 W/(m·K) | |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.18E+7 S/m Show Material materials with Conductividad eléctrica of 1.18E+7 S/m |
200.0 °C | 1.07E+7 S/m Show Material materials with Conductividad eléctrica of 1.07E+7 S/m | |
Resistividad eléctrica | 20.0 °C | 8.5E-8 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-8 Ω·m |
200.0 °C | 9.3E-8 Ω·m Show Material materials with Resistividad eléctrica of 9.3E-8 Ω·m | |
Chemical properties
Property | Value |
---|---|
Estaño | 3.5 - 4.5 % Show Material materials with Estaño of 3.5 - 4.5 % |
Fósforo | 0.01 - 0.4 % Show Material materials with Fósforo of 0.01 - 0.4 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |