Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Cobre pudelado
CEN/TS 13388 Grade CW112C R300, H070Bronce fosforado
EN 1652 Grade CuSn4 O60Bronce fosforado
EN 12166 Grade CuSn4 R330Bronce fosforado
EN 12166 Grade CuSn4 H01