EN 12166 Grade CuSn4 H230

View suppliers (9)
Want to keep this datasheet? Save it now in your required format

Description

CuSn4, mat. No. CW450K, is comparable to the DIN-make CuSn4, mat. No. 2.1016, acc. to DIN 17662 : 1983-12. The material is specified by a favorable combination of very good cold formability with strength and hardness. It is corrosion resistant, good soft and hard solderable and shows still good electrical conductivity. Properties of the CuSn-alloy are predominantly determined by the tin-content. The alloy is unhardenable, only work hardening is feasible. Tensile strength, yield point and hardness increase according to the rising cold forming grade, elongation after fracture decreases. Electrical and thermal conductivity are lower than for pure copper. Very high resistance to corrosion, particularly to atmospheric influences, seawater, sulfite liquor, carbonated and salted mine water. The alloys are stress corrosion-proof. Processing properties: warm forming: limited cold forming: very good machinability: moderately to hardly hard soldering: very good soft soldering: very good gas welding: medium arc welding: medium TIG-welding: good MIG_welding: good resistance welding: good electron beam welding: good sticking: suitable burnishing: good mechanical burnishing: good electrolytical/chemical burnishing: good galvanizing: very good suitability for dip tinning: very good Appliction: CuSn4 is predominantly used in the form of strips for all types of springs with mean requirements, such as connectors, electrographic springs for contacts and earthing contacts, clamp-connenctions for radio, TV and video, receptacles for electronical assemblies, for pushbutton shifting springs and locking clamps, spring rings as well as for textile machine components. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.7 - 8.9 g/cm³

Show Material materials with Densidad of 8.7 - 8.9 g/cm³

Mecánica

PropertyTemperatureValue

Coeficiente de Poisson

20.0 °C

0.34 [-]

Show Material materials with Coeficiente de Poisson of 0.34 [-]

Dureza Vickers

20.0 °C

230 [-]

Show Material materials with Dureza Vickers of 230 [-]

Módulo elástico

20.0 °C

120 GPa

Show Material materials with Módulo elástico of 120 GPa

Aplicaciones térmicas

PropertyTemperatureValue

Calor específico

20.0 °C

377 J/(kg·K)

Show Material materials with Calor específico of 377 J/(kg·K)

Coeficiente de dilatación térmica

100.0 °C

1.78E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.78E-5 1/K

200.0 °C

1.82E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.82E-5 1/K

300.0 °C

1.9E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K

650.0 °C

2.06E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.06E-5 1/K

800.0 °C

2.05E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.05E-5 1/K

Conductividad térmica

20.0 °C

90 - 100 W/(m·K)

Show Material materials with Conductividad térmica of 90 - 100 W/(m·K)

200.0 °C

120 W/(m·K)

Show Material materials with Conductividad térmica of 120 W/(m·K)

Unlock all property charts

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

1.18E+7 - 1.20E+7 S/m

Show Material materials with Conductividad eléctrica of 1.18E+7 - 1.20E+7 S/m

200.0 °C

1.07E+7 S/m

Show Material materials with Conductividad eléctrica of 1.07E+7 S/m

Unlock all property charts

Resistividad eléctrica

20.0 °C

8.5E-8 Ω·m

Show Material materials with Resistividad eléctrica of 8.5E-8 Ω·m

200.0 °C

9.3E-8 Ω·m

Show Material materials with Resistividad eléctrica of 9.3E-8 Ω·m

Unlock all property charts

Specific Electrical conductivity

21 % IACS

Show Material materials with Specific Electrical conductivity of 21 % IACS

Chemical properties

PropertyValue

Estaño

3.5 - 4.5 %

Show Material materials with Estaño of 3.5 - 4.5 %

Fósforo

0.01 - 0.4 %

Show Material materials with Fósforo of 0.01 - 0.4 %

Hierro

0.1 %

Show Material materials with Hierro of 0.1 %

Níquel

0.2 %

Show Material materials with Níquel of 0.2 %

Plomo

0.02 %

Show Material materials with Plomo of 0.02 %

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %