General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 - 8.9 g/cm³ Show Material materials with Densidad of 8.8 - 8.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 8 % Show Material materials with Elongación of 8 % |
Elongation A100 | 20.0 °C | 2 - 4 % Show Material materials with Elongation A100 of 2 - 4 % |
Elongation A11.3 | 20.0 °C | 4 - 6 % Show Material materials with Elongation A11.3 of 4 - 6 % |
Límite elástico Rp 0,2 | 20.0 °C | 610 MPa Show Material materials with Límite elástico Rp 0,2 of 610 MPa |
Módulo elástico | 20.0 °C | 138 GPa Show Material materials with Módulo elástico of 138 GPa |
Resistencia a la tracción | 20.0 °C | 730 MPa Show Material materials with Resistencia a la tracción of 730 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 300.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | |
Conductividad térmica | 20.0 °C | 192 - 239 W/(m·K) Show Material materials with Conductividad térmica of 192 - 239 W/(m·K) | |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Temperatura máx. de funcionamiento, largo | 0 - 350 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 350 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 2.50E+7 - 3.20E+7 S/m Show Material materials with Conductividad eléctrica of 2.50E+7 - 3.20E+7 S/m |
Specific Electrical conductivity | 43 % IACS Show Material materials with Specific Electrical conductivity of 43 % IACS |
Chemical properties
Property | Value |
---|---|
Berilio | 0.4 - 0.7 % Show Material materials with Berilio of 0.4 - 0.7 % |
Cobalto | 2 - 2.8 % Show Material materials with Cobalto of 2 - 2.8 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |