General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 110 [-] Show Material materials with Dureza Brinell of 110 [-] |
Dureza Vickers | 20.0 °C | 115 [-] Show Material materials with Dureza Vickers of 115 [-] |
Módulo de cizallamiento | 20.0 °C | 31 GPa Show Material materials with Módulo de cizallamiento of 31 GPa |
Módulo elástico | 20.0 °C | 84 GPa Show Material materials with Módulo elástico of 84 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Calor específico of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Coeficiente de dilatación térmica | 200.0 °C | 2.12E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.12E-5 1/K | |
Conductividad térmica | 20.0 °C | 126 W/(m·K) Show Material materials with Conductividad térmica of 126 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.64E+7 S/m Show Material materials with Conductividad eléctrica of 1.64E+7 S/m |
Resistividad eléctrica | 20.0 °C | 6.1E-8 Ω·m Show Material materials with Resistividad eléctrica of 6.1E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Cobre | 55 - 57 % Show Material materials with Cobre of 55 - 57 % |
Estaño | 0.3 % Show Material materials with Estaño of 0.3 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 1.6 - 3 % Show Material materials with Plomo of 1.6 - 3 % |