General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.1 - 8.12 g/cm³ Show Material materials with Densidad of 8.1 - 8.12 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 150 - 220 [-] Show Material materials with Dureza Brinell of 150 - 220 [-] | |
Dureza Vickers | 20.0 °C | 160 - 210 [-] Show Material materials with Dureza Vickers of 160 - 210 [-] | |
Límite elástico Rp 0,2 | 20.0 °C | 280 MPa Show Material materials with Límite elástico Rp 0,2 of 280 MPa | |
Módulo de cizallamiento | 23.0 °C | 40 GPa Show Material materials with Módulo de cizallamiento of 40 GPa | Typical for Wrought Copper Brass |
Módulo elástico | 20.0 °C | 93 GPa Show Material materials with Módulo elástico of 93 GPa | |
Resistencia a la tracción | 20.0 °C | 540 MPa Show Material materials with Resistencia a la tracción of 540 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.95E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.95E-5 1/K | |
300.0 °C | 2.04E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.04E-5 1/K | ||
Conductividad térmica | 20.0 °C | 63 W/(m·K) Show Material materials with Conductividad térmica of 63 W/(m·K) | |
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 7.80E+6 S/m Show Material materials with Conductividad eléctrica of 7.80E+6 S/m |
Specific Electrical conductivity | 13 - 13.4 % IACS Show Material materials with Specific Electrical conductivity of 13 - 13.4 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 1.3 - 2.3 % Show Material materials with Aluminio of 1.3 - 2.3 % |
Cobre | 56.5 - 59 % Show Material materials with Cobre of 56.5 - 59 % |
Estaño | 0.4 - 0.5 % Show Material materials with Estaño of 0.4 - 0.5 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 1.4 - 3 % Show Material materials with Manganeso of 1.4 - 3 % |
Níquel | 1 - 2 % Show Material materials with Níquel of 1 - 2 % |
Plomo | 0.2 - 0.8 % Show Material materials with Plomo of 0.2 - 0.8 % |
Silicona | 0.3 - 1.3 % Show Material materials with Silicona of 0.3 - 1.3 % |